Xenon Flash Lamp Annealing of Poly-Si Thin Films

Authors:

Abstract
We have investigated xenon (Xe) flash lamp annealing for the crystallization of amorphous silicon (a-Si) films for polycrystalline silicon (poly-Si) thin film transistors on glass substrates. The Xe flash lamp emits white light with a wavelength range of 400–800nm400–800nm for 40μs40μs , thereby instantaneously supplying the energy necessary to crystallize a-Si films to poly-Si films. The distance between electrodes in the lamp is 1000mm1000mm , the bore diameter is 10mm10mm , and the peak voltage is up to 20kV20kV . The sample structure is a-Si (50nm)∕SiOx(50nm)∕SiOx (100nm)(100nm) deposited on a glass substrate by plasma-enhanced chemical vapor deposition using SiH4SiH4 gas. An average grain size of 500nm500nm is obtained without substrate heating during Xe flash lamp annealing when the light energy density is 1.82J∕cm21.82J∕cm2 . The grain size is less than 50nm50nm at 1.55–1.78J∕cm21.55–1.78J∕cm2 , and a significant grain growth occurs at 1.82J∕cm21.82J∕cm2 . The light energy is absorbed by the whole a-Sia-Si film, because the Xe flash lamp emits light with a wide wavelength range of 400–800nm400–800nm . Therefore, when the light energy exceeds its threshold at which the a-Si film melting point is observed, a-Sia-Si films can be partially melted and subsequently crystallized at the top and bottom surfaces, thereby forming large-grain poly-Si.

This publication has 18 references indexed in Scilit: