Thermoelectric properties of Eu(Zn1−xCdx)2Sb2
- 25 September 2009
- journal article
- research article
- Published by Royal Society of Chemistry (RSC) in Dalton Transactions
- Vol. 39 (4) , 1101-1104
Abstract
The thermoelectric performance of EuZn2Sb2 and EuCd2Sb2 was optimized by mixed occupation of the transition metal position. Samples in the solid solution Eu(Zn1−xCdx)2Sb2 with the CaAl2Si2 -type crystal structure (space group m1) were prepared from the elements for compositions with x = 0, 0.1, 0.3, 0.5 and 1. The thermoelectric properties were investigated after densification of the products by spark plasma sintering (SPS). The samples show low electrical resistivity, high thermopower and a low lattice thermoconductivity. The highest ZT value of 1.06 at 650 K is obtained for x = 0.1.Keywords
This publication has 18 references indexed in Scilit:
- Synthesis and properties of CaCd2Sb2 and EuCd2Sb2Intermetallics, 2010
- Thermoelectric properties of p-type LiZnSb: Assessment of ab initio calculationsJournal of Applied Physics, 2009
- A new type of thermoelectric material, EuZn2Sb2The Journal of Chemical Physics, 2008
- Zintl phases for thermoelectric devicesDalton Transactions, 2007
- Automated Search for New Thermoelectric Materials: The Case of LiZnSbJournal of the American Chemical Society, 2006
- Nanostructuring, Compositional Fluctuations, and Atomic Ordering in the Thermoelectric Materials AgPbmSbTe2+m. The Myth of Solid SolutionsJournal of the American Chemical Society, 2005
- Nanostructured thermoelectric materialsJournal of Electronic Materials, 2005
- Disordered zinc in Zn4Sb3 with phonon-glass and electron-crystal thermoelectric propertiesNature Materials, 2004
- Cubic AgPb
m
SbTe 2+
m
: Bulk Thermoelectric Materials with High Figure of MeritScience, 2004
- Thin-film thermoelectric devices with high room-temperature figures of meritNature, 2001