Abstract
Growing interest in alternative alkaline activating systems and the increasing generation of polymer waste have encouraged the investigation of alternative material strategies for alkali-activated concrete. This study evaluates the fresh, mechanical and microstructural performance of ambient-cured ground granulated blast-furnace slag (GGBS)-based alkali-activated concrete produced using a laboratory-prepared pumice-derived silicate-containing activating component combined with 10 M sodium hydroxide (NaOH) and shredded recycled polypropylene (PP) as an alternative to the conventional 10 mm limestone aggregate fraction. Five alkali-activated formulations with mass-based activator-to-precursor (A/P) ratios ranging from 0.1–0.5 were evaluated alongside a Portland cement reference concrete. Workability, compressive strength development, splitting tensile strength, flexural failure load, hardened density and microstructural characteristics were evaluated. The alkali-activated formulations exhibited very low workability, with GL0 recording a slump of 5 mm and GL1–GL4 exhibiting zero measurable slump. Compressive strength increased with curing age, while formulations with higher A/P ratios generally exhibited lower strengths; at 90 days, values ranged from 10.66 MPa for GL0 to 7.64 MPa for GL4, compared with 39.43 MPa for the Portland cement reference. Similarly, 28-day splitting tensile strength ranged from 1.237 MPa for GL0 to 0.816 MPa for GL4. Qualitative visual and scanning electron microscopy observations revealed heterogeneous matrix features, visible pores and voids, and local PP particle separation and pull-out. Although the A/P ratios were calculated on a mass basis, their variation was accompanied by simultaneous changes in GGBS content, activating-liquid quantity, externally added water and superplasticizer dosage. Consequently, the observed trends are interpreted as formulation-dependent rather than as independently isolated effects of A/P. The results demonstrate that hardened ambient-cured GGBS-based concrete can be produced using the investigated combined pumice-derived activating system and recycled PP; however, the severe workability limitations, comparatively low mechanical performance and absence of equivalent activator and no-PP control formulations indicate that further optimization and controlled comparative investigation are required before engineering applicability can be established.

This publication has 30 references indexed in Scilit: