Abstract
High‐strength and high‐toughness polyethylene (PE) fibers are prepared by the melt‐spinning and subsequent drawing in the semimolten state of high‐density PE (HDPE) combined with ultrahigh‐molecular‐weight PE (UHMW‐PE). As‐spun fibers are prepared by the melt‐spinning of HDPE/UHMW‐PE blended powder with 0–30 wt% UHMW‐PE. The as‐spun fiber is drawn at 100 (solid state) and 130 °C (semimolten state). Well‐arranged stacked lamellae with highly oriented crystals are formed based on the difference in relaxation time for the drawn fiber with 30 wt% UHMW‐PE prepared at 130 °C in the semimolten state. This composite structure results in a PE fiber with high tensile strength (1.11 GPa) and high toughness (297 MJ m−3).
Funding Information
  • Ogasawara Foundation for the Promotion of Science and Engineering

This publication has 29 references indexed in Scilit: