Change in Electrical/Mechanical Properties of Plasma Polymerized Low Dielectric Constant Films after Etching in CF4/O2 Plasma for Semiconductor Multilevel Interconnects
Open Access
Abstract
As semiconductor chips have been integrated to enhance their performance, a low-dielectric-constant material, SiCOH, with a relative dielectric constant k ≤ 3.5 has been widely used as an intermetal dielectric (IMD) material in multilevel interconnects to reduce the resistance-capacitance delay. Plasma-polymerized tetrakis(trimethylsilyoxy)silane (ppTTMSS) films were created using capacitively coupled plasma-enhanced chemical vapor deposition with deposition plasma powers ranging from 20 to 60 W and then etched in CF4/O2 plasma using reactive ion etching. No significant changes were observed in the Fourier-transform infrared spectroscopy (FTIR) spectra of the ppTTMSS films after etching. The refractive index and dielectric constant were also maintained. As the deposition plasma power increased, the hardness and elastic modulus increased with increasing ppTTMSS film density. The X-ray photoelectron spectroscopy (XPS) spectra analysis showed that the oxygen concentration increased but the carbon concentration decreased after etching owing to the reaction between the plasma and film surface. With an increase in the deposition plasma power, the hardness and elastic modulus increased from 1.06 to 8.56 GPa and from 6.16 to 52.45 GPa. This result satisfies the hardness and elastic modulus exceeding 0.7 and 5.0 GPa, which are required for the chemical–mechanical polishing process in semiconductor multilevel interconnects. Furthermore, all leakage-current densities of the as-deposited and etched ppTTMSS films were measured below 10−6 A/cm2 at 1 MV/cm, which is generally acceptable for IMD materials.Keywords
Funding Information
- Basic Science Research Program through the National Research Foundation of Korea (NRF) (NRF-2019R1A6A1A10073079)
- Basic Science Research Program (NRF-2019R1A6A1A10073079)
This publication has 33 references indexed in Scilit:
- Non-porous ultra-low-kSiOCH (k= 2.3) for damage-free integration and Cu diffusion barrierJournal of Physics D: Applied Physics, 2013
- A robust k∼2.3 SiCOH low-k film formed by porogen removal with UV-cureMicroelectronic Engineering, 2007
- A global view of interconnectsMicroelectronic Engineering, 2006
- Chemical Bonding Structure of Low Dielectric Constant Si:O:C:H Films Characterized by Solid-State NMRJournal of the Electrochemical Society, 2005
- Structure of low dielectric constant to extreme low dielectric constant SiCOH films: Fourier transform infrared spectroscopy characterizationJournal of Applied Physics, 2003
- Comparison of techniques to characterise the density, porosity and elastic modulus of porous low-k SiO2 xerogel filmsMicroelectronic Engineering, 2002
- Infrared spectroscopy study of low-dielectric-constant fluorine-incorporated and carbon-incorporated silicon oxide filmsJournal of Applied Physics, 2001
- Hot-Filament Chemical Vapor Deposition of Organosilicon Thin Films from Hexamethylcyclotrisiloxane and OctamethylcyclotetrasiloxaneJournal of the Electrochemical Society, 2001
- Vibrational Structure of Monosubstituted OctahydrosilasesquioxanesThe Journal of Physical Chemistry B, 1997
- Investigation of SiO2 plasma enhanced chemical vapor deposition through tetraethoxysilane using attenuated total reflection Fourier transform infrared spectroscopyJournal of Vacuum Science & Technology A, 1995