Application of Preoxidation Treatment to Suppress60Co Deposition on Stainless Steel Surfaces of Boiling Water Reactor Primary Cooling Systems
Authors:
- 1 January 1985
- journal article
- research article
- Published by Taylor & Francis in Nuclear Science and Engineering
- Vol. 89 (1) , 61-69
Abstract
60Co accumulation on boiling water reactor (BWR) primary cooling pipings. To demonstrate the treatment effect, test specimens, which had been exposed to simulated BWR water in an autoclave (temperature, 286 °C; pH, 7; oxygen concentration, 200 ppb) for up to 200 h, were installed in the Hatch-2 inplant loop and their 60Co deposition amounts were compared with those of as-received specimens. Preoxidation treatment for 200 h resulted in deposits of about one-fourth those of as-received specimens. It was estimated that the maximum amount of 60Co deposited on primary piping during the entire plant operation life (30 yr) would be reduced to about one-half of that without preoxidation treatment if the 60Co concentration in the reactor water was constant.Keywords
This publication has 5 references indexed in Scilit:
- A Mechanism of Radioactive Corrosion Product Buildup on the Stainless Steel Surface Used in the Primary Cooling Systems of Boiling Water ReactorsNuclear Technology, 1982
- Removal of radioactive cobalt ion in high temperature water using titanium oxideNuclear Engineering and Design, 1979
- An Empirical Formula Predicting Shutdown Dose Rate of the Recirculation Pipes in Boiling Water ReactorsNuclear Science and Engineering, 1979
- Mass Transfer in the Contamination of Isothermal Steel SurfacesNuclear Science and Engineering, 1976
- The Transport of Radioactive Corrosion Products in High-Temperature Water II. The Activation of Isothermal Steel SurfacesNuclear Science and Engineering, 1976