Factors Influencing the Embrittlement of Cold Worked High Alloy Materials in H2S Environments
Authors:
- R. D. KaneRKR. D. Kane
- M. WatkinsMWM. Watkins
- D. F. JacobsDJD. F. Jacobs
- 1 September 1977
- journal article
- Published by Association for Materials Protection and Performance (AMPP) in Corrosion
- Vol. 33 (9) , 309-320
Abstract
The resistance of several high strength nickel and cobalt base alloys to embrittlement in aqueous H2S containing environments was examined. The alloys evaluated were Hastelloy Alloy C-276 and Alloy C-4, Inconel 625, and MP35N. All materials were received as tubing in the cold reduced condition and were subjected to various heat treatments ranging from 148 to 593 C (300 to 1100 F) for times from 10 minutes to over 500 hours. The effect on cracking susceptibility of: (1) cold working, (2) aging time and temperature, (3) sample orientation, (4) galvanic interaction with steel, and (5) environmental temperature and composition were determined. It was found that aging for very short periods at high temperature [482 to 593 C (900 to 1100 F)/10 minutes] or for longer times at low temperatures [148 to 204 C (300 to 400 F)/~500 hours] significantly reduced the resistance of these materials to hydrogen embrittlement. This behavior was greatly dependent on galvanic interaction with steel and on sample orientation. Failures were limited to samples that were coupled to steel and stressed in the transverse direction. No failures were observed in any longitudinally stressed specimens, even under very severe testing conditions, or in transversely stressed specimens without steel couples. Elevated temperature environments were beneficial in reducing the susceptibility to cracking and brittle failure. The results of these tests are discussed in terms of hydrogen embrittlement. Also, the metallurgical reactions occurring during aging are examined to determine their possible role in the hydrogen embrittlement behavior of these materials.Keywords
This publication has 7 references indexed in Scilit:
- Mechanism of yield strength enhancement in heavily cold rolled phosphor bronzeMetallurgical Transactions A, 1977
- Corrosion Testing of Highly Alloyed Materials For Deep, Sour Gas Well EnvironmentsJournal of Petroleum Technology, 1976
- The thermodynamic properties of the Fe-Ni-H ternary systemActa Metallurgica, 1976
- Directionality of Hydrogen Embrittlement in Hot-Rolled Steel PlateTransactions of the Japan Institute of Metals, 1971
- Permeation of hydrogen through steel by electrochemical transfer—I. Influence of catalytic poisonsElectrochimica Acta, 1966
- Intercrystalline fracture in hydrogen-charged nickelActa Metallurgica, 1965
- The influence of hydrogen on the plastic deformation ductility, and fracture of nickel in tensionActa Metallurgica, 1963