Dry Sliding Behavior of an Aluminum Alloy after Innovative Hard Anodizing Treatments
Open Access
Abstract
This work evaluates the dry sliding behavior of anodic aluminum oxides (AAO) formed during one traditional hard anodizing treatment (HA) and two golden hard anodizing treatments (named G and GP, respectively) on a EN AW-6060 aluminum alloy. Three different thicknesses of AAO layers were selected: 25, 50, and 100 μm. Prior to wear tests, microstructure and mechanical properties were determined by scanning electron microscopy (VPSEM/EDS), X-ray diffractometry, diffuse reflectance infrared Fourier transform (DRIFT-FTIR) spectroscopy, roughness, microhardness, and scratch tests. Wear tests were carried out by a pin-on-disc tribometer using a steel disc as the counterpart material. The friction coefficient was provided by the equipment. Anodized pins were weighed before and after tests to assess the wear rate. Worn surfaces were analyzed by VPSEM/EDS and DRITF-FTIR. Based on the results, the GP-treated surfaces with a thickness of 50 μm exhibit the lowest friction coefficients and wear rates. In any case, a tribofilm is observed on the wear tracks. During sliding, its detachment leads to delamination of the underlying anodic aluminum oxides and to abrasion of the aluminum substrate. Finally, the best tribological performance of G- and GP-treated surfaces may be related to the existence of a thin Ag-rich film at the coating/aluminum substrate interfaces.Keywords
This publication has 53 references indexed in Scilit:
- Failure analysis of worn valve train components of a four-cylinder diesel engineEngineering Failure Analysis, 2018
- Tribological Behavior of a Cr2O3 Ceramic Coating/Steel Couple Under Dry Sliding and Heavy Loading ConditionsJournal of Materials Engineering and Performance, 2018
- Effect of relative humidity and applied loads on the tribological behaviour of a steel/Cr2O3-ceramic couplingWear, 2013
- Improving sliding and abrasive wear behaviour of cast A356 and wrought AA7075 aluminium alloys by plasma electrolytic oxidationMaterials & Design (1980-2015), 2010
- Comparative study of mechanical and tribological properties of alumina coatings formed on aluminium in various conditionsMaterials & Design (1980-2015), 2009
- HVOF-sprayed WC–CoCr coatings on Al alloy: Effect of the coating thickness on the tribological propertiesWear, 2009
- The effect of sulphuric anodisation of aluminium alloys on contact problemsSurface and Coatings Technology, 2006
- Growth peculiarities of aluminum anodic oxide at high voltages in diluted phosphoric acidJournal of Crystal Growth, 2001
- Sealing of anodic films obtained in oxalic acid bathsSurface and Coatings Technology, 2000
- Porous anodic alumina: fabrication, characterization and applicationsThin Solid Films, 1997