Dissolution kinetics of a sodium borosilicate glass in Tris buffer solutions: impact of Tris concentration and acid (HCl/HNO 3 ) identity
- 8 July 2021
- journal article
- research article
- Published by Royal Society of Chemistry (RSC) in Physical Chemistry Chemical Physics
- Vol. 23 (30) , 16165-16179
Abstract
Understanding the corrosion behavior of glasses in near-neutral environments is crucial for many technologies including glasses for regenerative medicine and nuclear waste immobilization. To maintain consistent pH values throughout experiments in the pH = 7 to 9 regime, buffer solutions containing tris(hydroxymethyl)aminomethane (“Tris”, or sometimes called THAM) are recommended in ISO standards 10993-14 and 23317 for evaluating biomaterial degradation and utilized throughout glass dissolution behavior literature—a key advantage being the absence of dissolved alkali/alkaline earth cations (i.e. Na+ or Ca2+) that can convolute experimental results due to solution feedback effects. Although Tris is effective at maintaining the solution pH, it has presented concerns due to the adverse artificial effects it produces while studying glass corrosion, especially in borosilicate glasses. Therefore, many open questions still remain on the topic of borosilicate glass interaction with Tris-based solutions. We have approached this topic by studying the dissolution behavior of a sodium borosilicate glass in a wide range of Tris-based solutions at 65 °C with varied acid identity (Tris–HCl vs. Tris–HNO3), buffer concentration (0.01 M to 0.5 M), and pH (7–9). The results have been discussed in reference to previous studies on this topic and the following conclusions have been made: (i) acid identity in Tris-based solutions does not exhibit a significant impact on the dissolution behavior of borosilicate glasses, (ii) ∼0.1 M Tris-based solutions are ideal for maintaining solution pH in the absence of obvious undesirable solution chemistry effects, and (iii) Tris–boron complexes can form in solution as a result of glass dissolution processes. The complex formation, however, exhibits a distinct temperature-dependence, and requires further study to uncover the precise mechanisms by which Tris-based solutions impact borosilicate glass dissolution behavior.Keywords
Funding Information
- Division of Materials Research (1507131)
- Division of Materials Research (2034871)
- Office of Science (DE-AC05-00OR22725)
- Nuclear Energy University Program (DE-NE0008597)
This publication has 65 references indexed in Scilit:
- Modeling glass corrosion with GRAALnpj Materials Degradation, 2018
- Corrosion of the International Simple Glass under acidic to hyperalkaline conditionsnpj Materials Degradation, 2018
- Non-destructive characterization of corroded glass surfaces by spectroscopic ellipsometryJournal of Non-Crystalline Solids, 2018
- Composition effects on synthetic glass alteration mechanisms: Part 1. ExperimentsChemical Geology, 2010
- Experimental determination of the effect of the ratio of B/Al on glass dissolution along the nepheline (NaAlSiO4)–malinkoite (NaBSiO4) joinGeochimica et Cosmochimica Acta, 2010
- An experimental study of the dissolution rates of simulated aluminoborosilicate waste glasses as a function of pH and temperature under dilute conditionsApplied Geochemistry, 2008
- Experimentally determined dissolution kinetics of Na-rich borosilicate glass at far from equilibrium conditions: Implications for Transition State TheoryGeochimica et Cosmochimica Acta, 2008
- Aluminoborosilicate waste glass dissolution under alkaline conditions at 40°C: implications for a chemical affinity-based rate equationEnvironmental Chemistry, 2008
- Aluminum speciation and equilibria in aqueous solution: V. Gibbsite solubility at 50°C and pH 3–9 in 0.1 molal NaCl solutions (a general model for aluminum speciation; analytical methods)Geochimica et Cosmochimica Acta, 1994
- Percolation Phenomenon for Dissolution of Sodium Borosilicate Glasses in Aqueous SolutionsJournal of the American Ceramic Society, 1991