Abstract
To achieve high-quality, groove-free single-pass welding of 8 mm thick 5052-H112 aluminum alloy, this study investigates the effects of oscillating laser welding (OLW) and laser-arc hybrid welding (LAHW) using ER5356 and 5052 filler wires. The research focuses on addressing critical challenges: insufficient penetration, porosity sensitivity, and Mg burn-off. Results demonstrate that the OLW process with ER5356 filler wire achieves superior weld stability, full penetration, and the highest relative density. This condition yielded a tensile strength of 182.4 MPa and 13.1% elongation, reaching 82.7% of the base metal strength. In contrast, 5052 filler or LAHW processes resulted in insufficient penetration and reduced ductility. Microstructural analysis indicates that OLW produces a narrower heat-affected zone and finer, equiaxed grains. EBSD characterization further reveals higher grain boundary density and significantly weakened texture intensity in OLW-ER5356 joints. Fracture analysis confirms a transition from ductile-brittle mixed modes in other conditions to dominant microvoid coalescence in OLW-ER5356. The superior performance is fundamentally attributed to a synergistic effect: laser oscillation regulates molten pool dynamics to stabilize the keyhole and refine the solidification structure, while high-Mg filler compensates for alloy vaporization to maintain solid-solution strengthening. This study provides a high-efficiency, groove-free solution for joining medium-thick aluminum alloys, offering significant insights into the metallurgical control of Al-Mg alloys.

This publication has 25 references indexed in Scilit: