Spark Plasma Sintering (SPS) of NASICON Ceramics
Authors:
- 1 February 2004
- journal article
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 87 (2) , 305-307
Abstract
Spark plasma sintering (SPS) method was used to obtain dense NASICON ceramics with a high‐electrical conductivity, which was compared with conventional solid‐state sintering. The fully dense NASICON was achieved at a relatively low‐sintering temperature of 1100°C, whereas the apparent density of the specimen prepared by conventional sintering was 74% of the theoretical density. The highest conductivity of 1.8 × 10 −3 Scm −1 at 25°C, which is comparable to the best value reported, was achieved using the SPS process. Considering the phase, density, and microstructure, it appears that there is more room for improved conductivity by controlling the amount of monoclinic zirconia and the resistive grain‐boundary glass phase.Keywords
This publication has 21 references indexed in Scilit:
- Humidity Influence on the CO 2 Response of Potentiometric Sensors Based on NASICON Pellets with New Compositions, Na 3 Zr
2−(
x
/4)
Si
2−
x
P
1+
x
O 12 ( x = 1.333)Journal of the American Ceramic Society, 2002
- Use of NASICON/Na2CO3 system for measuring CO2Sensors and Actuators B: Chemical, 2000
- Development of a NASICON-based amperometric carbon dioxide sensorSensors and Actuators B: Chemical, 2000
- Particular features of admittance spectra of polycrystalline NASICON samplesSolid State Ionics, 1999
- Potentiometric Gas Sensors for Oxidic GasesJournal of Electroceramics, 1998
- Optimization of NASICON composition for Na+ recognitionSensors and Actuators B: Chemical, 1997
- Dependence of the properties of Nasicons on their composition and processingSolid State Ionics, 1987
- Sol-gel routes leading to nasicon ceramicsCeramics International, 1986
- Phase transformation in Na1+xSixZr2P3−xO12 compoundsMaterials Research Bulletin, 1979
- Crystal structures and crystal chemistry in the system Na1+xZr2SixP3−xO12Materials Research Bulletin, 1976