Bond strength between fibre posts and composite resin cores: effect of post surface silanization

Authors:

Abstract
Aim  To evaluate the tensile bond strength between two different composite resin cores and (ClearfilTMCore, MultiCore® Flow) and fibre posts (DT Light Post®), with and without silanization of the post surface.Methodology  Forty fibre posts were shortened to a length of 15 mm. Specimens were then produced by covering the upper 3 mm of the posts with standardized composite core build‐ups. The bonding surfaces of twenty posts were treated with silane coupling agent (Monobond‐S). Four experimental groups were formed: G1: ClearfilTMCore; G2: Monobond‐S + ClearfilTMCore; G3: MultiCore® Flow; G4: Monobond‐S + MultiCore® Flow. Each post was positioned upright in a post centric device with moulds to ensure standardized shapes of the abutments. After tensile bond strength testing, the type of failure at the interface was determined. The results obtained were compared using an unpaired sample t‐test.Results  The mean tensile bond strengths and standard deviations were [MPa] 10.08 ± 0.92 for ClearfilTMCore, 10.47 ± 1.05 for ClearfilTMCore + silane; 6.65 ± 0.79 for MultiCore® Flow and 6.91 ± 0.83 for MultiCore® Flow + silane. Statistical analysis revealed that ClearfilTMCore achieved significantly higher bond strengths than MultiCore® Flow (P < 0.0001). Post silanization had no significant effect. All tested specimens had an adhesive failure mode.Conclusion  Type of composite had a significant effect on tensile bond strength. Silanization of fibre post surfaces had no effect on core retention.

This publication has 18 references indexed in Scilit: