Plating on magnesium alloy diecastings

Authors:

Abstract
Magnesium alloy diecasting AZ91CC,* AZ61CC, AZ91HC* and AZ71HC were electroplated using three proprietary pretreatment sequences which incorporated conventional zincate immersion processes. Satisfactory peel adhesion in excess of 7.7KNm−1 was achieved on AZ61CC using a sequence designated “WCM” which used the same zincate solution as the Norsk Hydro process. The comparatively low adhesion achieved on the AZ91HC was due to its poor surface quality as cast. Growth of deposits was monitored using a strip and analysis technique and the morphology of the various deposits studied using scanning electron microscopy. The three pretreatment sequences resulted in different surface responses for the alloys but all alloys behaved in a similar manner in a particular sequence with regard to potential/time curves and the rate of zinc deposition. Although the minimum levels of adhesion, using the WCM sequence, varied from 7.72KNm−1 for alloy AZ61CC to 1.54KNm−1 for alloy AZ91HC, all the alloys revealed ductile failure characteristics in the surface layer of the substrate after peel testing. Plated magnesium alloys exhibited good corrosion resistance when appropriately pretreated and overplated with adequate nickel chromium coatings. The immersion zinc layer was not preferentially attacked when pits penetrated to the coating/substrate interface. Hemispherical pits formed and attack on the substrate was severe. Of the pretreatment sequences investigated, the WCM one was the most promising with respect to peel adhesion and corrosion behavior. *CC Cold Chamber *HC Hot Chamber

This publication has 6 references indexed in Scilit: