Enhancement of Tech‐Sil25 Maxillofacial Silicone Mechanical Properties after Artificial Weathering through Addition of Nanoparticles
Open Access
- 1 January 2022
- journal article
- research article
- Published by Wiley in International Journal of Dentistry
- Vol. 2022 (1) , 4082168
Abstract
Purpose. To evaluate the effect of nanosilica and nanoalumina addition in Tech‐sil25 maxillofacial silicone before and after exposure to artificial weathering conditions. Materials and Methods. A total of 144 samples were divided into four groups, a control group (n = 12) and three test groups, nanosilica (NS) (n = 36), nanoalumina (NA) (n = 36), and a hybrid nanoparticle (HySA) (n = 60) at different weight percentages (1, 2, and 3 wt. %) was added to Tech‐sil25. Samples were exposed to artificial weathering for 100 hours, and subjected to characterizations involving tear strength, shore A hardness, roughness, and tensile strength tests. The data were analyzed using descriptive and inferential statistics using a one‐way ANOVA test to determine the level of significance between the groups. Results. After 100 hours of artificial weathering, the one‐way ANOVA result shows a highly significant increase in tensile and tear strengths with a minimal increase in hardness and roughness observed in samples containing 2% nanosilica (NS) followed by hybrid nanoparticle (HySA) of 1% nanoalumina (NA) + 1% nanosilica (NS) compared with a control group and other groups. Conclusions. The addition of nanosilica (NS), nanoalumina (NA), and a hybrid nanoparticle (HySA) to the Tech‐sil25 maxillofacial silicone improved its mechanical properties. The combination of several filler reinforcements is essential for enhancing silicone’s antiaging properties of silicone and maintaining some of its mechanical properties to prolong the service life.Keywords
Funding Information
- Universiti Sains Malaysia (8014034)
This publication has 16 references indexed in Scilit:
- Studying some mechanical properties of maxillofacial silicone elastomer before and after incorporation of intrinsic pigments and artificial agingFuture Dental Journal, 2018
- Evaluation of some mechanical properties of a new silicone elastomer for maxillofacial prostheses after addition of intrinsic pigmentsThe Saudi Dental Journal, 2018
- Effect of Nano Silicon Dioxide Addition on Some Properties of Heat Vulcanized Maxillofacial Silicone ElastomerIOSR Journal of Pharmacy and Biological Sciences, 2017
- Effect of addition of pigments and opacifier on the hardness, absorption, solubility and surface degradation of facial silicone after artificial ageingPolymer Degradation and Stability, 2012
- Color stability of pigmented maxillofacial silicone elastomer: Effects of nano-oxides as opacifiersJournal of Dentistry, 2010
- Effect of nano-oxide concentration on the mechanical properties of a maxillofacial silicone elastomerThe Journal of Prosthetic Dentistry, 2008
- Development of a new poly(dimethylsiloxane) maxillofacial prosthetic materialJournal of Biomedical Materials Research Part B: Applied Biomaterials, 2003
- Evaluation of Various Reinforcements for Maxillofacial Silicone ElastomersJournal of Biomaterials Applications, 1994
- Use of medical-grade methyl triacetoxy silane crosslinked silicone for facial prosthesesThe Journal of Prosthetic Dentistry, 1982
- PROSTHETIC RECONSTRUCTION OF NOSE AND EAR WITH A LATEX COMPOUNDJAMA, 1941