Forgeability and die-forging forming of direct chill casting Mg–Nd–Zn–Zr magnesium alloy
Authors:
- Xingwei ZhengXZXingwei Zheng
- Jie DongJDJie Dong
- Dongdi YinDYDongdi Yin
- Wencai LiuWLWencai Liu
- Fenghua WangFWFenghua Wang
- Li JinLJLi Jin
- Wenjiang DingWDWenjiang Ding
- 1 June 2010
- journal article
- Published by Elsevier in Materials Science and Engineering: A
- Vol. 527 (16-17) , 3690-3694
Abstract
No abstract availableKeywords
This publication has 16 references indexed in Scilit:
- Microstructure and mechanical properties of Mg–4Al–4Nd–0.5Zn–0.3Mn alloyMaterials Science and Engineering: A, 2009
- Effects of heat treatments on the microstructures and mechanical properties of Mg–3Nd–0.2Zn–0.4Zr (wt.%) alloyMaterials Science and Engineering: A, 2008
- Hot forgeability and die-forging forming of semi-continuously cast AZ70 magnesium alloyMaterials Science and Engineering: A, 2008
- Flow stress and microstructure evolution of semi-continuous casting AZ70 Mg-alloy during hot compression deformationTransactions of Nonferrous Metals Society of China, 2008
- Comparison of the corrosion behaviour in 5% NaCl solution of Mg alloys NZ30K and AZ91DJournal of Applied Electrochemistry, 2007
- Deformation behaviour of an AJ50 magnesium alloy at elevated temperaturesMaterials Science and Engineering: A, 2007
- Effect of heat treatment on corrosion and electrochemical behaviour of Mg–3Nd–0.2Zn–0.4Zr (wt.%) alloyElectrochimica Acta, 2007
- Forgeability of Mg–Al–Zn magnesium alloys in hot and warm closed die forgingJournal of Materials Processing Technology, 2006
- Deformation behaviour of Mg–0.7 wt.% Nd alloyJournal of Alloys and Compounds, 2004
- A two-step processing route for achieving a superplastic forming capability in dilute magnesium alloysScripta Materialia, 2002