Influence of the Rear Interface on Composition and Photoluminescence Yield of CZTSSe Absorbers: A Case for an Al2O3 Intermediate Layer
Authors:
- Antonio Cabas-VidaniACAntonio Cabas-Vidani
- Leo ChoubracLCLeo Choubrac
- José A. MárquezJMJosé A. Márquez
- Thomas UnoldTUThomas Unold
- Roland ScheerRSRoland Scheer
- Hu LiHu Li
- Klaus LeiferKlaus Leifer
- Evgeniia GilshteinEGEvgeniia Gilshtein
- Ayodhya N. TiwariATAyodhya N. Tiwari
- Yaroslav E. RomanyukYRYaroslav E. Romanyuk
Open Access
- 18 April 2021
- journal article
- research article
- Published by American Chemical Society (ACS) in ACS Applied Materials & Interfaces
- Vol. 13 (16) , 19487-19496
Abstract
The rear interface of kesterite absorbers with Mo back contact represents one of the possible sources of nonradiative voltage losses (ΔVoc,nrad) because of the reported decomposition reactions, an uncontrolled growth of MoSe2, or a nonoptimal electrical contact with high recombination. Several intermediate layers (IL), such as MoO3, TiN, and ZnO, have been tested to mitigate these issues, and efficiency improvements have been reported. However, the introduction of IL also triggers other effects such as changes in alkali diffusion, altered morphology, and modifications in the absorber composition, all factors that can also influence ΔVoc,nrad. In this study, the different effects are decoupled by designing a special sample that directly compares four rear structures (SLG, SLG/Mo, SLG/Al2O3, and SLG/Mo/Al2O3) with a Na-doped kesterite absorber optimized for a device efficiency >10%. The IL of choice is Al2O3 because of its reported beneficial effect to reduce the surface recombination velocity at the rear interface of solar cell absorbers. Identical annealing conditions and alkali distribution in the kesterite absorber are preserved, as measured by time-of-flight secondary ion mass spectrometry and energy-dispersive X-ray spectroscopy. The lowest ΔVoc,nrad of 290 mV is measured for kesterite grown on Mo, whereas the kesterite absorber on Al2O3 exhibits higher nonradiative losses up to 350 mV. The anticipated field-effect passivation from Al2O3 at the rear interface could not be observed for the kesterite absorbers prepared by the two-step process, further confirmed by an additional experiment with air annealing. Our results suggest that Mo with an in situ formed MoSe2 remains a suitable back contact for high-efficiency kesterite devices.Keywords
Funding Information
- Svenska Forskningsr?det Formas (2019-01538)
- H2020 Leadership in Enabling and Industrial Technologies (720907)
- Shandong University
This publication has 54 references indexed in Scilit:
- Hole mobility enhancement of Cu-deficient Cu1.75Zn(Sn1−xAlx)Se4 bulksJournal of Solid State Chemistry, 2013
- Single crystal X-ray structure investigation of Cu2ZnSnSe4Surface Engineering and Applied Electrochemistry, 2013
- Inhibiting the absorber/Mo-back contact decomposition reaction in Cu2ZnSnSe4 solar cells: the role of a ZnO intermediate nanolayerJournal of Materials Chemistry A, 2013
- Multinuclear (67Zn, 119Sn and 65Cu) NMR spectroscopy – an ideal technique to probe the cationic ordering in Cu2ZnSnS4 photovoltaic materialsPhysical Chemistry Chemical Physics, 2013
- A Detrimental Reaction at the Molybdenum Back Contact in Cu2ZnSn(S,Se)4 Thin-Film Solar CellsJournal of the American Chemical Society, 2012
- Surface passivation of Cu(In,Ga)Se2 using atomic layer deposited Al2O3Applied Physics Letters, 2012
- Chemical Insights into the Instability of Cu2ZnSnS4 Films during AnnealingChemistry of Materials, 2011
- The Consequences of Kesterite Equilibria for Efficient Solar CellsJournal of the American Chemical Society, 2011
- Silicon surface passivation by ultrathin Al2O3 films synthesized by thermal and plasma atomic layer depositionPhysica Status Solidi (RRL) – Rapid Research Letters, 2010
- Vegard’s lawPhysical Review A, 1991