Increased Elasticity Modulus of Polymeric Materials Is a Source of Surface Alterations in the Human Body
Open Access
- 16 April 2021
- journal article
- research article
- Published by MDPI AG in Journal of Functional Biomaterials
- Vol. 12 (2) , 24
Abstract
The introduction of alloplastic materials (meshes) in hernia surgery has improved patient outcome by a radical reduction of hernia recurrence rate, but discussion about the biocompatibility of these implanted materials continues since observations of surface alterations of polypropylene and other alloplastic materials were published. This study intends to investigate if additives supplemented to alloplastic mesh materials merge into the solution and become analyzable. Four polypropylene and one polyester alloplastic material were incubated in different media for three weeks: distilled water, saline solution, urea solution, formalin, and hydrogen peroxide. No swelling or other changes were observed. Infrared spectroscopy scanning of incubated alloplastic materials and NMR studies of extracted solutions were performed to investigate loss of plasticizers. The surface of the mesh materials did not show any alterations independent of the incubation medium. FT-IR spectra before and after incubation did not show any differences. NMR spectra showed leaching of different plasticizers (PEG, sterically hindered phenols, thioester), of which there was more for polypropylene less for polyester. This could be the reason for the loss of elasticity of the alloplastic materials with consecutive physically induced surface alterations. A mixture of chemical reactions (oxidative stress with additive leaching from polymer fiber) in connection with physical alterations (increased elasticity modulus by loss of plasticizers) seem to be a source of these PP and PE alterations.Keywords
This publication has 38 references indexed in Scilit:
- Materials characterization of explanted polypropylene, polyethylene terephthalate, and expanded polytetrafluoroethylene composites: Spectral and thermal analysisJournal of Biomedical Materials Research Part B: Applied Biomaterials, 2010
- Foreign body reaction to biomaterialsSeminars in Immunology, 2008
- Characterization of Heavyweight and Lightweight Polypropylene Prosthetic Mesh Explants From a Single PatientSurgical Innovation, 2007
- Materials characterization of explanted polypropylene hernia meshesJournal of Biomedical Materials Research Part B: Applied Biomaterials, 2007
- Comparative investigation of alloplastic materials for hernia repair with improved methodologySurgical Endoscopy, 2005
- Effect of moisture content on mechanical properties, thermal and structural stability and extrudate texture of poly(vinyl chloride)/wood sawdust compositesPolymer International, 2004
- Study of the thermal evolution of the cyclic-oligomer formation in a cyclic-oligomer-free PETJournal of Polymer Science Part A: Polymer Chemistry, 2000
- Glass Wool–H2O2/CoCl2 test system for in vitro evaluation of biodegradative stress cracking in polyurethane elastomersJournal of Biomedical Materials Research, 1995
- Human plasma α2‐macroglobulin promotes in vitro oxidative stress cracking of pellethane 2363‐80A: In vivo and in vitro correlationsJournal of Biomedical Materials Research, 1993
- Morphological instability of poly(ethylene terephthalate) cyclic oligomer crystalsJournal of Materials Science, 1985