Abstract
Various phenomena encountered in metal fatigue with hydrogen-material interaction are investigated. Slip bands observed in grains of hydrogen-charged (H-charged) specimens under fatigue test are localized and discrete. On the other hand, various cross slip bands are observed in grains of uncharged specimens. Basically a similar mechanism becomes dominant in the neighborhood of a propagating fatigue crack tip. The crack growth rate of a H-charged specimen is higher than that of an uncharged specimen. This is due to the difference in crack opening and closure behavior caused by the difference in slip deformation behavior between H-charged and uncharged specimens. Therefore, hydrogen content at the crack tip strongly influences fatigue crack growth. At the same time, a definite "time" is necessary for hydrogen diffusion and concentration to the fatigue crack tip and accordingly the hydrogen content at the crack tip is controlled by how long the crack tip stays in the region of hydrogen concentration. Thus, test frequency (strain rate) has an extremely important effect on the result of metal fatigue in the presence of hydrogen. This paper overviews the recent experimental results obtained in the Research Center for Hydrogen Industrial Use and Storage, AIST (HYDROGENIUS) and discusses the fatigue mechanism caused by hydrogen.