Abstract
High-density polyethylene (HDPE) has attracted attention as an alternative material for marine structures because of its chemical resistance, processability, and recyclability. However, internal pores formed during extrusion welding can reduce weld quality and mechanical performance. This study investigated pore formation mechanisms in HDPE extrusion welds by considering material throughput, filler wire storage condition, and artificial defect volume fraction. Porosity increased from 0.06% to 0.37% as material throughput increased from 0.96 to 2.00 kg/h and slightly decreased to 0.33% at 2.60 kg/h. Under these process conditions, tensile strength changed within approximately 1.49%, whereas elongation decreased more clearly with increasing porosity. In contrast, residual surface moisture on the filler wire caused severe pore formation and reduced tensile strength by approximately 55.53%. Artificial defect tests also confirmed that increasing internal defect volume directly reduced tensile strength. Overall, controlling material throughput and removing surface moisture are essential for improving HDPE extrusion weld quality.
Funding Information
  • Korea Institute of Marine Science & Technology Promotion
  • Ministry of Oceans and Fisheries (RS-2026-25527726)
  • Korea Institute of Industrial Technology (EH-260010)
  • Korea Institute of Industrial Technology (PEH26100)

This publication has 20 references indexed in Scilit: