V2O5-Assisted Low-Temperature Sintering and Microwave Dielectric Properties of (1 − x)Li2.08TiO3–xLi2ZnTi3O8 (x = 0.3−0.7) Ceramics for LTCC Applications
Open Access
Abstract
A new composite microwave–dielectric system, (1 − x)Li2.08TiO3-xLi2ZnTi3O8 (x = 0.3–0.7), was systematically investigated to identify the optimal composition for low-temperature co-fired ceramic (LTCC) applications by correlating sintering behavior, microstructural evolution, and microwave–dielectric properties. Although the undoped compositions exhibited excellent intrinsic dielectric performance, they required sintering at 1100 °C, making them incompatible with Ag-based LTCC processing. Among the investigated formulations, 0.6Li2.08TiO3–0.4Li2ZnTi3O8 was identified as the most suitable base composition. To reduce the sintering temperature, 0.3–1.0 wt.% V2O5 was introduced as a sintering aid, enabling densification at 900 °C for 30 min (97.0% relative density) while preserving the coexistence of Li2.08TiO3 and Li2ZnTi3O8 without XRD-detectable secondary phases. Microstructural observations indicated that V2O5 promoted liquid-phase sintering, leading to enhanced densification and Li2.08TiO3-selective abnormal grain coarsening without altering the intrinsic permittivity. Complementary dilatometry provided process-level evidence for this liquid-phase sintering mechanism: large total shrinkage at 900 °C (≈ −17–19%), earlier / with lowered by ~250 °C, and an increased , collectively supporting 900 °C/30 min as the practical firing window. The optimized 0.6Li2.08TiO3–0.4Li2ZnTi3O8 composition containing 0.3 wt.% V2O5 exhibits excellent microwave–dielectric properties ( = 23.32, Q × f = 68,400 GHz, and = −1.55 ppm/°C). Higher V2O5 contents (>0.3 wt.%) caused a gradual reduction in Q × f due to increasing microstructural non-uniformity. Ag co-firing tests confirmed electrode stability with no interfacial reactions at 900 °C for 30 min. Overall, 0.3 wt.% V2O5-assisted 0.6Li2.08TiO3–0.4Li2ZnTi3O8 provides a practical sub-950 °C processing window that satisfies key LTCC requirements, including moderate permittivity, high Q × f, near-zero , and compatibility with Ag electrodes.
Keywords
Funding Information
- Soonchunhyang University Research Fund
- Korea Institute for Advancement of Technology (KIAT) Grant
- Korea Institute for Advancement of Technology (KIAT) Grant (P0012453)
This publication has 45 references indexed in Scilit:
- All-ceramic array patch for 5G signal enhancement based on B-site substituted zinc-cobalt molybdate low temperature co-fired ceramicsChemical Engineering Journal, 2023
- Spinel-olivine microwave dielectric ceramics with low sintering temperature and high quality factor for 5 GHz wi-fi antennasApplied Materials Today, 2020
- Microwave dielectric properties of the low-temperature-fired Li2ZnTi3O8–Li2TiO3 ceramics for LTCC applicationsJournal of Materials Science: Materials in Electronics, 2018
- Effect of V2O5 Addition on the Phase Composition of Bi5FeTi3O15 Ceramic and RF/Microwave Dielectric PropertiesJournal of Electronic Materials, 2017
- Enhanced Sinterability and Microwave Dielectric Performance of (1 − x)ZnAl2O4-xLi4/3Ti5/3O4 CeramicsJournal of Electronic Materials, 2016
- Structural Dependence of Microwave Dielectric Properties of Spinel-Structured Li2ZnTi3O8 Ceramic: Crystal Structure Refinement and Raman Spectroscopy StudyJournal of Electronic Materials, 2015
- Microstructures and microwave dielectric properties of Li2ZnTi3O8 ceramics prepared by reaction-sintering processJournal of Materials Science: Materials in Electronics, 2014
- Towards rational design of low-temperature co-fired ceramic (LTCC) materialsJournal of Advanced Ceramics, 2012
- The effect of sintering atmosphere on the microwave dielectric properties of V2O5 doped BiNbO4 ceramicsCeramics International, 2004
- Improvements of sintering and dielectric properties on Bi2O3–ZnO–Nb2O5 pyrochlore ceramics by V2O5 substitutionCeramics International, 2004