Abstract
This research examines the use of a single-screw extrusion process to produce 3D printing filament from virgin polypropylene (PP-V) and recycled polypropylene (PP-R). The extrusion-based production of polypropylene filaments is the subject of the research, with an emphasis on assessing the effects of material type and process variables on filament quality. The primary issue addressed is the challenge of creating dimensionally stable and flawless 3D printing filament from recycled polypropylene, which is prone to internal void development and diameter irregularity as a result of thermal degradation. According to the research findings, under the same processing circumstances, PP-V consistently yields filaments with bigger and more stable diameters than PP-R. Using PP-V at a barrel temperature of 200°C, a puller speed of 12 rpm, and fan cooling produced the best results, with an average diameter of 1.71 mm, nearly the normal filament diameter of 1.75 mm. PP-R filaments, on the other hand, showed voids in their cross-sections at higher temperatures and reached a maximum diameter of 1.57 mm. These findings are explained by the fact that virgin polypropylene has greater thermal stability and viscosity, whereas recycled polypropylene undergoes partial thermal degradation during reprocessing, which results in decreased melt strength and void formation. The methodical comparison of material condition, barrel temperature, puller speed, and cooling media, along with cross-sectional measurements and statistical analysis, is a unique aspect of this research. The results apply to additive manufacturing applications focused on the circular economy since optimal performance is attained under regulated extrusion temperatures, low puller speeds, and air cooling.
Funding Information
  • Udayana University

This publication has 25 references indexed in Scilit: