Abstract
A calcium titanium phosphate glass–ceramic for use as a dental material with excellent chemical durability was derived from a mother glass with a small amount of fluorine. The laser Raman spectroscopic analysis showed that 35CaO–10CaF2–30P2O5–25TiO2 glass, as the nominal composition, consists of ortho‐, pyro‐, and meta‐phosphate groups. On heating the glass at 865°C, orthophosphate crystals, such as fluorine‐containing oxyapatite (Ca10(PO4)6(O,F2)) and the Nasicon‐type phase (CaTi4(PO4)6), were preferentially precipitated; the apatite particles of several tens of nanometers in size were embedded in the CaTi4(PO4)6 phase. The pale bluish color of the glass–ceramic indicated that titanium ions were included in the residual glassy phase. When the glass–ceramic was treated with dilute hydrochloric acid, only the apatite particles at the surface were leached out, while no CaTi4(PO4)6 phase was etched; the dissolution of the glass–ceramic was effectively controlled. Almost no dissolution of ions from the glass–ceramic occurred in water. It was suggested that the behavior is a result of the microstructure of the glass–ceramic, which consists of crystalline and glassy phases with excellent chemical durability.

This publication has 15 references indexed in Scilit: