Fabrication of Two Dimensional Silicon Carbide Fiber-Reinforced Silicon Carbide Composite by Electrophoretic Deposition and Hot-Pressing
- 1 August 2007
- journal article
- Published by Trans Tech Publications, Ltd. in Key Engineering Materials
- Vol. 352, 77-80
Abstract
In this study, Tyranno SA fiber cloth was coated with carbon black and SiC powder containing sintering aids by means of electrophoretic deposition method, and SiC/SiC composites with three different fiber volume fractions were fabricated using the Tyranno SA cloth by hot-pressing at 1700oC. The sufficient formation of the SiC matrix between each fiber could be observed. The composite fractured in non-brittle manner, and bending strength decreased with increasing fiber volume fraction. The crack propagation and fracture behavior depended on the fiber volume fraction. These differences in bending strength and fracture behavior would be caused by the difference in the interfacial bonding between fiber cloth and the matrix.Keywords
This publication has 3 references indexed in Scilit:
- Improvement of the mechanical properties of hot-pressed silicon-carbide-fiber-reinforced silicon carbide composites by polycarbosilane impregnationComposites Science and Technology, 2001
- Room- and High-Temperature Thermal Conductivity of Silicon Carbide Fiber-Reinforced Silicon Carbide Composites with Oxide Sintering Additives.Journal of the Ceramic Society of Japan, 2001
- Processing and microstructure of silicon carbide fiber-reinforced silicon carbide composite by hot-pressingJournal of Nuclear Materials, 1998