Creep rupture induced silica-based nanofibers formed on fracture surfaces of Ti3SiC2
- 1 November 2005
- journal article
- Published by Springer Nature in Journal of Materials Research
- Vol. 20 (11) , 2895-2897
Abstract
After creep failure at 1300 °C, silica-based nanofibers with diameters of ∼250 nm and lengths of up to a few tens of microns were observed on the fracture surfaces of Ti3SiC2. A possible mechanism for the formation of these fibers is proposed.Keywords
This publication has 10 references indexed in Scilit:
- Tensile creep of coarse-grained Ti3SiC2 in the 1000–1200°C temperature rangeJournal of Alloys and Compounds, 2003
- Oxidation of Ti3SiC2 at 1000°C in AirOxidation of Metals, 2003
- Long Time Oxidation Study of Ti[sub 3]SiC[sub 2], Ti[sub 3]SiC[sub 2]/SiC, and Ti[sub 3]SiC[sub 2]/TiC Composites in AirJournal of the Electrochemical Society, 2003
- Ternary Compound Ti3SiC2: Part I. Pulse Discharge Sintering SynthesisMATERIALS TRANSACTIONS, 2002
- Mechanical properties of polycrystalline Ti3SiC2 at ambient and elevated temperaturesActa Materialia, 2001
- The MN+1AXN phases: A new class of solidsProgress in Solid State Chemistry, 2000
- The Topotactic Transformation of Ti3SiC2 into a Partially Ordered Cubic Ti ( C 0.67Si0.06 ) Phase by the Diffusion of Si into Molten CryoliteJournal of the Electrochemical Society, 1999
- Oxidation Of Ti3SiC2 in AirJournal of the Electrochemical Society, 1997
- Chemically vapor deposited Ti3SiC2Materials Research Bulletin, 1987
- Die Kristallstruktur von Ti3SiC2—ein neuer Komplexcarbid-TypMonatshefte für Chemie - Chemical Monthly, 1967