Effect of coating thickness on thermal stresses in tungsten-coated optical fibers

Authors:

Abstract
This study investigates the effect of coating thickness on the thermal stresses in tungsten-coated optical fibers. Theoretical results indicate that the maximum normal stress in the tungsten coating decreases with increasing coating thickness. However, the maximum shear stress at the interface of the glass fiber and tungsten coating increases. Eight samples of tungsten-coated optical fibers with coating thicknesses of 58, 75, 101, 128, 158, 383, 557, and 1013 nm, respectively, are immersed in liquid nitrogen for one day. Experimental results show that thermal stresses will either break or delaminate the tungsten coating. The crack density decreases with increased coating thickness, while the delaminated area of tungsten coating increases. The theoretical results can explain the break and delamination of the tungsten coating in the optical fiber. To minimize the break and delamination of the tungsten coatings in the optical fibers, the optimal thickness of the tungsten coating is about 158 nm.

This publication has 14 references indexed in Scilit: