Mechanical and Biocompatibility Properties of Sintered Titanium Powder for Mimetic 3D-Printed Bone Scaffolds
Authors:
Open Access
- 16 March 2022
- journal article
- research article
- Published by American Chemical Society (ACS) in ACS Omega
- Vol. 7 (12) , 10340-10346
Abstract
A composite comprising Ti and NaCl powders was sintered similar to a three-dimensional (3D)-printed patient-customized artificial bone scaffold. Additionally, a proper microstructure of the mimetic scaffold and the optimum processing parameters for its development were analyzed. The mechanical properties of the metal-based porous-structured framework used as an artificial bone scaffold were an optimum replacement for the human bone. Thus, it was confirmed that patient-customized scaffolds could be manufactured via 3D printing. The 3D-printed mimetic specimens were fabricated by a powder-sintering method using Ti for the metal parts, NaCl as the pore former, and polylactic acid as the biodegradable binder. Scanning electron microscopy (SEM) images showed that pores were formed homogeneously, while X-ray computed tomography confirmed that open pores were generated. The porosity and pore size distribution were measured using a mercury porosimeter, while the flexural strength and flexural elastic modulus were calculated using the three-point bending test. Based on these measurements, a pore-former content of 15 vol % optimized the density and flexural strength to 2.52 g cm–2 and 283 MPa, respectively, similar to those of the actual iliac bone. According to the 3D-printing production method, a selective laser-sintering process was applied for the fabrication of the mimetic specimen, and it was determined that the microstructure and properties similar to those of previous metal specimens could be achieved in the as-prepared specimen. Additionally, a decellularized extracellular matrix (dECM) was used to coat the surfaces and interiors of the specimens for evaluating their biocompatibilities. SEM image analysis indicated that the adipose-derived stem cells grew evenly inside the pores of the coated specimens, as compared with the bulky Ti specimens without the dECM coating. The doubling time at 65% was measured at 72, 75, and 83 h for specimens with pore-former contents of 5, 10, and 15 vol %, respectively. The doubling time without the pore former was 116 h. As compared with the specimens without the pore former (73 h), 15% of the dECM-coated specimens showed a doubling time of 64%, measured at 47 h.Keywords
Funding Information
- National Research Foundation of Korea (2017M3A9E2093907, 2020R1A2C1012838)
This publication has 40 references indexed in Scilit:
- Biomecánica y hueso (y II): ensayos en los distintos niveles jerárquicos del hueso y técnicas alternativas para la determinación de la resistencia óseaRevista de Osteoporosis y Metabolismo Mineral, 2013
- Establishment of process parameters for producing Al-foam by dissolution and powder sintering methodMaterials & Design (1980-2015), 2011
- Decellularized matrices for tissue engineeringExpert Opinion on Biological Therapy, 2010
- Chondrogenic and osteogenic differentiations of human bone marrow-derived mesenchymal stem cells on a nanofibrous scaffold with designed pore networkBiomaterials, 2009
- Problem of Stress Shielding and Improvement to the Hip Implant Designs: A ReviewJournal of Medical Sciences, 2007
- The mechanical properties and osteoconductivity of hydroxyapatite bone scaffolds with multi-scale porosityBiomaterials, 2007
- A bioactive titanium foam scaffold for bone repairActa Biomaterialia, 2005
- Tissue Engineering--Current Challenges and Expanding OpportunitiesScience, 2002
- Processing of biocompatible porous Ti and MgScripta Materialia, 2001
- Hydroxylapatite coating of porous implants improves bone ingrowth and interface attachment strengthJournal of Biomedical Materials Research, 1992