A porous ceramic preform was fabricated by printing a powder blend of TiC, TiO2, and dextrin. The presintered preforms contained a bimodal pore size distribution with intra‐agglomerate pores (d50≈0.7 μm) and inter‐agglomerate pores (d50≈30 μm), which were subsequently infiltrated by aluminum melt spontaneously in argon above 1050°C. A redox reaction at 1400°C resulted in the formation of dense Ti–Al–O–C composites mainly composed of Ti3AlC2, TiAl3, Al, and Al2O3, which attained a bending strength of 320 MPa, a Young's modulus of 184 GPa, and a Vicker's hardness of 2.5 GPa.