Determination of the Forward Dissolution Rate for International Simple Glass in Alkaline Solutions
Authors:
Open Access
- 5 January 2017
- journal article
- Published by Springer Nature in MRS Advances
- Vol. 2 (12) , 661-667
Abstract
The International Simple Glass (ISG) is considered as reference benchmark glass and is used in the frame of an international collaboration for the study of the dissolution mechanisms of high-level vitrified nuclear waste.In this work the forward dissolution rate of the ISG was determined in different alkaline solutions, as a simulation of the disposal conditions foreseen by the Belgian concept for geological disposal of vitrified waste. The determination of the forward dissolution rate was done by measuring the Si released from the glass in solution in tests performed at 30 °C in four different KOH solutions with pH varying from 9 to 14 and in artificial cementitious water at pH 13.5.The forward dissolution rates determined for the ISG in high pH solutions are in good agreement with the results obtained for a lower pH range.The rates obtained in this study, moreover, were compared with the rates measured in the same conditions for SON68 glass from a previous work. The values obtained for the two glasses are comparable in artificial cementitious water and in KOH at moderately alkaline pH. At higher pH, ISG glass shows a lower forward dissolution rate with respect to SON68 (0.20 g•m−2•d for ISG and 0.35 g•m−2 d for SON68 at pH 14).Keywords
This publication has 19 references indexed in Scilit:
- Resumption of Alteration at High Temperature and pH: Rates Measurements and Comparison with Initial RatesProcedia Materials Science, 2014
- Formation of alteration products during dissolution of vitrified ILW in a high-pH calcium-rich solutionJournal of Nuclear Materials, 2013
- Initial Dissolution Rate of the International Simple Glass as a Function of pH and Temperature Measured Using Microchannel Flow‐Through Test MethodInternational Journal of Applied Glass Science, 2013
- An international initiative on long-term behavior of high-level nuclear waste glassMaterials Today, 2013
- Dissolution of vitrified wastes in a high-pH calcium-rich solutionJournal of Nuclear Materials, 2013
- Determination of the Forward Rate of Dissolution for SON68 and PAMELA Glasses in Contact With Alkaline SolutionsMRS Proceedings, 2008
- Effects of Iron and pH on Glass Dissolution RateMRS Proceedings, 2002
- Hydrolysis of R7T7 Nuclear Waste Glass in Dilute Media: Mechanisms and Rate as a function of PhMRS Proceedings, 1990
- Dissolution Kinetics of a Simple Analogue Nuclear Waste Glass as a Function of Ph, Time and TemperatureMRS Proceedings, 1989