Abstract
An infiltration-reaction (IR) method can fabricate a dense MgB $_{2}$ bulk under ambient pressure, thus being a promising method for mass production. However, the IR-processed MgB $_{2}$ bulks are known to contain the unreacted Mg and B and the intermediate product, Mg $_{2}$ B $_{25}$ , which degrades the trapped field, $B_\mathrm{T}$ , and critical current density, $J_\mathrm{c}$ , of the bulks. To expedite the creation of the MgB $_{2}$ phase during the IR process, we prepared the refined B powder by ball-milling and fabricated the MgB $_{2}$ bulks by the IR method. We achieved both improved $B_\mathrm{T}$ and $J_\mathrm{c}$ for the MgB $_{2}$ bulks made from the ball-milled B powders with sub-micron size. The microstructural analysis suggested that these results originated from the refinement of MgB $_{2}$ grains and the increase of the volume fraction of MgB $_{2}$ phase. The refinement of the starting B powder is quite effective to enhance the magnetic properties for the IR-processed MgB $_{2}$ bulks.
Funding Information
  • JST A-STEP (JPMJTM20JP)
  • JSPS KAKENHI (JP18K04920, JP21H01788)

This publication has 18 references indexed in Scilit: