Abstract
Nanocyrstalline LaAlO3:Sm3+LaAlO3:Sm3+ phosphors were prepared through a Pechini-type sol-gel process. X-ray diffraction (XRD), field-emission scanning electron microscopy (FE-SEM), photoluminescence, and cathodoluminescence (CL) spectra were utilized to characterize the synthesized phosphors. XRD results reveal that the sample begins to crystallize at 600°C600°C , and pure LaAlO3LaAlO3 phase can be obtained at 700°C700°C . FE-SEM images indicate that the Sm3+Sm3+ -doped LaAlO3LaAlO3 phosphors are composed of aggregated spherical particles with sizes ranging from 40to80nm40to80nm . Under the excitation of UV light (245nm)(245nm) and low-voltage electron beams (1–3kV)(1–3kV) , the Sm3+Sm3+ -doped LaAlO3LaAlO3 phosphors show the characteristic emissions of the Sm3+Sm3+ ( G5∕24–H5∕26G5∕24–H5∕26 , H7∕26H7∕26 , H9∕26H9∕26 transitions) with a yellow color. The CL intensity (brightness) of the Sm3+Sm3+ -doped LaAlO3LaAlO3 phosphor is higher than that of the commercial product [Zn(Cd)S:Ag+][Zn(Cd)S:Ag+] (yellow) to some extent.

This publication has 32 references indexed in Scilit: