Effect of NaCl concentration on corrosion of Al alloy during repeated wet–dry cycle tests at 323 K—comparing with corrosion in immersion tests‐
- 4 December 2015
- journal article
- research article
- Published by Wiley in Surface and Interface Analysis
- Vol. 48 (8) , 767-774
Abstract
Corrosion of 4043‐Al alloy was examined by repeated wet–dry cycle tests with NaCl solutions at 323 K, and compared with immersion test corrosion in 0.2–5.5 kmol/m 3 NaCl solutions. The Al alloy specimens after the immersion tests for 86.4 ks (1 day) or 604.8 ks (7 days) showed preferential dissolution of the aluminum matrix around Si‐phase compounds, and the dissolution was more remarkable at lower NaCl concentrations. Mass loss of the specimens after the 604.8‐ks immersion was also higher at lower NaCl concentrations. In the repeated wet–dry cycle tests, a 20 mm 3 droplet of 0.2–5.5 kmol/m 3 NaCl solution was initially dripped on the specimens, and left for 690 s to allow the drying up of the droplet, resulting in solid NaCl precipitation. Then, the dissolution and precipitation of NaCl were repeated a further 149 times by dripping 20‐mm 3 pure water at 690‐s intervals. The specimens after the 150 cycles showed different corrosion modes at the center and edge of the droplets. At the edge, 40–80 × 10 −6 pits/m 2 of 20–50 µm diameter had formed, showing more corrosion with higher NaCl concentration droplets, and at the droplet center, the corrosion showed preferential dissolution of the aluminum matrix around the Si‐phases, similar to the situation in the immersion tests. Copyright © 2015 John Wiley & Sons, Ltd.Keywords
This publication has 18 references indexed in Scilit:
- Corrosion of metals and salt hydrates used for thermochemical energy storageRenewable Energy, 2015
- Corrosion of Al-Alloys during Dry/Wet-Repeating Atmospheres with Pure Water and NaCl SolutionCorrosion Engineering, 2014
- Synergistic effects of Cl − and Cu 2+ ions on corrosion of pure Al and Al alloys in aqueous solutions at 363 KSurface and Interface Analysis, 2013
- Corrosion of Al and Al Alloys in Cl- and Cu2+ Ion-containing Solutions at 363 KCorrosion Engineering, 2013
- Effect of Cl− and Cu2+ Ions on Corrosion of 4043-Al Alloy in Aqueous Solutions at High-TemperatureJournal of The Surface Finishing Society of Japan, 2012
- INVESTIGATION ON THE RELATIONSHIP BETWEEN OCCUPANTS' INDIVIDUAL DIFFERENCE AND AIR-CONDITIONING USAGE DURING NIGHTTIME IN SUMMERJournal of Environmental Engineering (Transactions of AIJ), 2008
- Sequence of steps in the pitting of aluminum by chloride ionsCorrosion Science, 2003
- Pitting corrosion of aluminumCorrosion Science, 1999
- Residential Solar-Powered Air Conditioner.IEEJ Transactions on Industry Applications, 1993
- Accelerated Atmospheric Corrosion Testing Using a Cyclic Wet/Dry Exposure Test: Aluminum, Galvanized Steel, and SteelCorrosion, 1987