Bending moments of zirconia and titanium abutments with internal and external implant–abutment connections after aging and chewing simulation
- 28 March 2011
- journal article
- research article
- Published by Wiley in Clinical Oral Implants Research
- Vol. 23 (1) , 12-18
Abstract
Objectives: To test the fracture load of zirconia abutments with different types of implant–abutment connections after chewing simulation and to compare their bending moments to internally connected identical titanium abutments. Materials and methods: Forty‐eight identical customized zirconia abutments with different implant–abutment connections were fabricated for four different test groups: one‐piece internal implant–abutment connection (BL; Straumann Bonelevel), two‐piece internal implant–abutment connection (RS; Nobel Biocare Replace Select), external implant–abutment connection (B; Brånemark MK III), two‐piece internal implant–abutment connection (SP; Straumann Standard Plus). Twelve titanium abutments with one‐piece internal implant–abutment connection (T; Straumann Bonelevel) served as control group. After aging by means of thermocycling (5–50°C, 120 s) and chewing simulation (1,200,000 cycles, 49 N load, 1.67 Hz), static load was applied at a 30° angle to the palatal surface until failure. Bending moments were calculated for comparison of the groups. Data were analyzed descriptively and by performing the Kruskal–Wallis test with Bonferroni correction. Results: The mean bending moments of the abutments were 714.1 ± 184.9 N cm (T), 331.7 ± 57.8 N cm (BL), 429.7 ± 62.8 N cm (RS), 285.8 ± 64.4 N cm (B) and 379.9 ± 59.1 N cm (SP). The bending moments of control group T were significantly higher than those of all other groups. The values of group RS were significantly higher than those of group B but within the value range of groups SP and BL. Conclusion: The bending moments of the different tested types of zirconia abutments vary with different implant–abutment connections after chewing simulation. The use of a secondary metallic component might have a beneficial influence on the stability of zirconia abutments. To cite this article: Truninger TC, Stawarczyk B, Leutert CR, Sailer TR, Hämmerle CHF, Sailer I. Bending moments of zirconia and titanium abutments with internal and external implant–abutment connections after aging and chewing simulation. Clin. Oral Impl. Res. 23, 2012; 12–18. doi: 10.1111/j.1600‐0501.2010.02141.xKeywords
This publication has 22 references indexed in Scilit:
- An overview of zirconia ceramics: Basic properties and clinical applicationsJournal of Dentistry, 2007
- In vitro fracture strength and thermal shock resistance of metal-ceramic crowns with cast and machined AuTi frameworksThe Journal of Prosthetic Dentistry, 2007
- Fracture resistance of single‐tooth implant‐supported all‐ceramic restorations after exposure to the artificial mouthJournal of Oral Rehabilitation, 2006
- Fracture resistance of single-tooth implant-supported all-ceramic restorations: An in vitro studyThe Journal of Prosthetic Dentistry, 2006
- What future for zirconia as a biomaterial?Biomaterials, 2006
- Survival rate, fracture strength and failure mode of ceramic implant abutments after chewing simulationJournal of Oral Rehabilitation, 2005
- Strength, fracture toughness and microstructure of a selection of all-ceramic materials. Part II. Zirconia-based dental ceramicsDental Materials, 2004
- Fatigue resistance of two implant/abutment joint designsThe Journal of Prosthetic Dentistry, 2002
- An in vitro evaluation of the strength of an internal conical interface compared to a butt joint interface in implant designClinical Oral Implants Research, 1997
- A 3-year follow-up study on single implant treatmentJournal of Dentistry, 1993