Abstract
Introduction: The study aims to develop an effective method for selective reduction of iron from high-phosphorus oolitic ore, enabling the subsequent separation of low-phosphorus metallic iron and high-phosphorus slag. The approach involves fluxing the ore with calcium oxide (CaO) to stabilize phosphorus and facilitate its removal. Methods: The oolitic iron ore was fluxed with CaO to achieve a basicity of 2.0, then subjected to oxidative roasting at 1200 °C in a Nabertherm muffle furnace to convert iron phosphates into stable calcium phosphates. Solid-phase reduction was performed in a laboratory Tamman furnace at 1000 °C under a CO atmosphere. Final smelting was conducted at 1600 °C in a vertical Nabertherm furnace to achieve liquid-phase separation of metal and slag. X-ray diffraction and micro-X-ray spectral analysis were used for phase characterization. Results: CO selectively reduced iron to metallic form in both fluxed and non-fluxed samples, while phosphorus remained in the oxide phase. In fluxed samples, phosphorus was primarily present as calcium and aluminum phosphates, and iron was fully metallized. In non-fluxed samples, partial iron reduction occurred with residual phosphorus in iron, calcium, and aluminum phosphates. Upon smelting, non-fluxed ore formed a single melt with 0.1 wt.% phosphorus, whereas fluxed samples yielded separate metal and slag phases, with 0.3 wt.% phosphorus retained in the slag. Discussion: The results confirm that fluxing promotes the formation of stable calcium phosphates, preventing phosphorus reduction and enabling efficient Fe–P separation. The selective reduction of iron by CO was kinetically controlled and did not reduce phosphorus compounds. Compared to non-fluxed treatment, fluxing significantly improves the separation of phosphorus into slag during smelting. Conclusion: This study demonstrates a two-stage process for effective dephosphorization of high-phosphorus oolitic iron ores. Key contributions include the identification of phosphorus stabilization mechanisms via CaO fluxing, successful selective reduction of iron by CO, and development of a method for producing low-phosphorous metal and high-phosphorous slag. The approach offers a promising route for processing refractory iron ores.Keywords
This publication has 20 references indexed in Scilit:
- Direct Reduction of High-Phosphorus Oolitic Hematite: Quantifying Phosphorus Migration and RecoveryMetallurgical and Materials Transactions B, 2024
- Ultrasonic treatment of high phosphorus Australian iron ore finesMinerals Engineering, 2022
- Characterisation of phosphorus and other impurities in goethite-rich iron ores – Possible P incorporation mechanismsMinerals Engineering, 2019
- Characterization studies on Agbaja iron ore: a high-phosphorus content oreSN Applied Sciences, 2019
- Spatio-temporal distribution and tectonic settings of the major iron deposits in China: An overviewOre Geology Reviews, 2014
- Recovery of iron from high phosphorus oolitic iron ore using coal-based reduction followed by magnetic separationInternational Journal of Minerals, Metallurgy and Materials, 2013
- Removal of Phosphorus From High Phosphorus Iron Ores by Selective HCl Leaching MethodJournal of Iron and Steel Research International, 2011
- Phosphorus Removal of High Phosphorus Iron Ore by Gas-Based Reduction and Melt SeparationJournal of Iron and Steel Research International, 2010
- Mobilization of phosphorus from iron ore by the bacterium Burkholderia caribensis FeGL03Minerals Engineering, 2009
- Examples of biogenic support of mineralization in two oolitic iron ores—lorraine (France) and gara djebilet (Algeria)Sedimentary Geology, 1987