Abstract
This research aims to investigate the microstructure evolution and related mechanical properties of Mg-9.5Gd-0.8Zn-0.5Zr alloys with different Y contents (x = 0, 1, 2, and 3wt%). The effects of different heat treatment conditions on these alloys were investigated. The results show that the initial microstructure of the as-cast alloy without Y is composed of α-Mg matrix and Mg5Gd phase. Additional phases such as Mg24(Gd,Y)5 and Mg24Y5 appeared with the increase of Y content. After homogenization treatment, these phases are transformed into high temperature stable 14H-LPSO phase. It is noteworthy that the precipitation of the β′ phases in peak-aged alloys significantly enhances the strength, while the addition of Y enhances the plasticity. The peak-aged Mg-9.5Gd-0.8Zn-0.5Zr-2Y alloy exhibits the best mechanical properties, and the ultimate tensile strength, yield strength and elongation are 313MPa, 211MPa and 6.51%, respectively.

This publication has 27 references indexed in Scilit: