Abstract
The effects of secondary phases on microwave dielectric properties were investigated for CaSmAlO 4 ‐based ceramics with bulk compositions of (2+2 x )CaO·(1− x )Sm 2 O 3 ·Al 2 O 3 ( x =−0.10, −0.05, 0, 0.05, 0.10) and (2+2 x )CaO·Sm 2 O 3 ·Al 2 O 3 ( x =0.02, 0.04). In dense ceramics with bulk compositions of (2+2 x )CaO·(1− x )Sm 2 O 3 ·Al 2 O 3 , Ca 3 Al 2 O 6 ( x >0) and SmAlO 3 ( x ≤0) secondary phases were observed. Moreover, Sm 2 O 3 was detected for x x =0.2. The secondary phases of Ca 3 Al 2 O 6 and SmAlO 3 increased the dielectric loss (tan δ) and the temperature coefficient of the resonant frequency (τ f ). In dense ceramics with bulk compositions of (2+2 x )CaO·Sm 2 O 3 ·Al 2 O 3 ( x =0.02, 0.04), the additional CaO eliminated the SmAlO 3 secondary phase and led to the formation of a CaSmAl 3 O 7 secondary phase. Microwave dielectric properties were greatly improved for ceramics with bulk compositions of (2+2 x )CaO·Sm 2 O 3 ·Al 2 O 3 ( x =0.02, 0.04): ɛ r =19.2; Q × f =120 000–120 400 GHz; τ f =−10 to −9 ppm/°C.

This publication has 19 references indexed in Scilit: