In static high‐temperature (300°C) corrosion tests of mild steel in dilute solutions, both the corrosion rate and morphology of the generated oxide film were observed to vary in a reproducible and presumably correlatable fashion as the concentration increased. A transitory corrosion rate minimum was found ; there was at this same point a change in the structure of the oxide film, with a compact, randomly oriented, apparently continuous film giving way to a crystallographic surface oxide as the critical concentration was exceeded. The activation energy for corrosion differed depending on which oxide type prevailed, being 5–8 kcal/mol for the noncrystallographic oxide and 16 kcal/mol for the crystallographic. The transformation is thought to be basically a transition between passive and active corrosion states.