Thermal stability of the engineered interfaces in Wf/W composites
- 2 March 2012
- journal article
- Published by Springer Nature in Journal of Materials Science
- Vol. 47 (11) , 4706-4715
Abstract
No abstract availableKeywords
This publication has 13 references indexed in Scilit:
- Shear debonding behavior of a carbon-coated interface in a tungsten fiber-reinforced tungsten matrix compositeJournal of Nuclear Materials, 2011
- Aluminum-based composites reinforced with SiC particles and NiTi fibers: influence of fiber dimensions and aging time on mechanical propertiesJournal of Materials Science, 2010
- A study on the synthesis of nanostructured WC–10 wt% Co particles from WO3, Co3O4, and graphiteJournal of Materials Science, 2010
- Feasibility study of a tungsten wire-reinforced tungsten matrix composite with ZrOx interfacial coatingsComposites Science and Technology, 2010
- Interfacial fracture behavior of tungsten wire/tungsten matrix composites with copper-coated interfacesMaterials Science and Engineering: A, 2010
- Effects of environment on creep behavior of two oxide/oxide ceramic–matrix composites at 1200 °CJournal of Materials Science, 2008
- Influence of different physical factors on microstructure and properties of magnetron sputtered amorphous carbon filmsThin Solid Films, 2001
- Mechanics of the fiber pushout testMechanics of Materials, 1993
- Shear‐Lag Analysis of Fiber Push‐Out (Indentation) Tests for Estimating Interfacial Friction Stress in Ceramic‐Matrix CompositesJournal of the American Ceramic Society, 1988
- Analysis of the effect of embedded fibre length on fibre debonding and pull-out from an elastic matrixJournal of Materials Science, 1984