Design and development of submerged arc welding fluxes using TiO2-SiO2-CaO and SiO2-CaO-Al2O3 flux system
Authors:
- 4 September 2018
- journal article
- research article
- Published by SAGE Publications in Proceedings of the Institution of Mechanical Engineers, Part E: Journal of Process Mechanical Engineering
- Vol. 233 (4) , 739-762
Abstract
Submerged arc welding is widely used in pipeline manufacturing due to higher efficiency as compared to the other welding processes. In present study, TiO2-SiO2-CaO and SiO2-CaO-Al2O3–based submerged arc welding fluxes were developed for joining of linepipe steel. Twenty-one fluxes were formulated based on mixture design methodology. Fluxes were analysed using X-ray florescence (XRF), thermogravimetric, differential-scanning calorimetry, Hot-disc and X-ray diffraction (XRD) techniques. The structural behaviour of rutile basic fluxes were analysed using Fourier transformed infrared spectroscopy (FTIR). Thermo-gravimetric analysis and differential scanning calorimetry were performed from 25 ℃ to 900 ℃ in order to determine the thermal stability and change in enthalpy of fluxes. Thermal conductivity, thermal diffusivity and specific heat of each flux were evaluated by hot disc technique. The density and grain fineness number for flux particles was evaluated at room temperature. Multi objective optimisation was performed to derive the optimised flux formulations. Individual effect of all the mixture constituents is rarely observed on the physicochemical properties of fluxes as compared to the binary and ternary mixture effects. The binary compositions significantly affect the density. TiO2-CaO is the most effective binary mixture which has increasing effect on density while all remaining binary mixture constituents have decreasing effect. The weight loss of fluxes observed during thermogravimetric analysis is affected by binary and ternary mixture constituents. Both binary and ternary flux mixtures affect change in enthalpy observed during differential scanning calorimetry. SiO2.Al2O3 is the only most effective binary mixture constituent of flux having increasing effect on thermal conductivity. Binary mixture constituents TiO2.CaF2, SiO2.Al2O3 and CaO.Al2O3 are the most effective and having synergistic effect on thermal diffusivity.Keywords
This publication has 22 references indexed in Scilit:
- Modeling flux chemistry for submerged arc weldments of high-strength low-alloy steelProceedings of the Institution of Mechanical Engineers, Part B: Journal of Engineering Manufacture, 2014
- Effect of Powder Shape and Size on Mechanical Properties of Al Thin Plate Formed by Compression Shearing Method at Room TemperatureProcedia Engineering, 2014
- Effects of nucleating agents on crystallization and microstructure of fluorophlogopite mica-containing glass–ceramicsJournal of Materials Science, 2013
- Review on effect of flux composition on its behavior and bead geometry in submerged arc welding (SAW)Journal of Mechanical Engineering Research, 2013
- Investigation on flux design for submerged arc welding of high-strength low-alloy steelProceedings of the Institution of Mechanical Engineers, Part B: Journal of Engineering Manufacture, 2013
- Influence of Y2O3 on structural and optical properties of SiO2–BaO–ZnO–xB2O3–(10−x) Y2O3 glasses and glass ceramicsJournal of Non-Crystalline Solids, 2011
- Combined effect of flux and welding parameters on chemical composition and mechanical properties of submerged arc weld metalJournal of Materials Processing Technology, 2006
- Critical evaluation and optimization of the thermodynamic properties and phase diagrams of the CaO-Al2O3, Al2O3-SiO2, and CaO-Al2O3-SiO2 systemsMetallurgical Transactions B, 1993
- Chemical reactions during submerged arc welding with FeO-MnO-SiO2 fluxesMetallurgical Transactions B, 1985
- Phase Equilibria in the System CaO‐TiO 2 –SiO 2Journal of the American Ceramic Society, 1955