Solution heat treatment of 319 aluminium alloy containing ~0.5wt% Mg. Part 1- solidification and tensile properties
Authors:
- 29 November 1996
- journal article
- research article
- Published by Taylor & Francis in International Journal of Cast Metals Research
- Vol. 9 (4) , 195-211
Abstract
The present work was carried out to establish the appropriate solution heat treatment for 319 aluminium alloy containing ~0.5 wt% Mg. Several solution treatments (single-stage and two-stage) were tried, where the single-stage treatment comprised 8–24 h at 480–520°C/water quench (60°C), while the two-stage treatment comprised 12h at 510°C/12h at 510–540°C/lowering the temperature to 480°C/water quench (60°C). It was found that addition of magnesium in quantities up to ~0.5 wt% results in (i) partial transformation of the β-Al5FeSi phase into Al8Mg3FeSi6, (ii) precipitation of Mg2Si, and (iii) precipitation of an Al5Mg8 Cu2Si6 phase. The melting temperature of this latter phase is about 508°C, i.e. 10°C below that reported for low Mg alloys. Modification with strontium refines the eutectic silicon particles with no noticeable effects on Cu or Mg reactions. Magnesium up to ~0.5 wt% contributes to both strength parameters by about 75% and to alloy ductility by about 15%. The two-stage solution heat treatment consisting of 12 h at 510°C (to dissolve all the copper-containing phases), followed by 12 h at 540°C (to dissolve β-Al5FeSi needles as well as coarsen the eutectic silicon particles in order to increase the area of the Al matrix) is a powerful heat treatment for low Mg, low intermetallic alloys. Addition of Mg necessitates lowering the second solution temperature to 520°C (to avoid incipient melting of the Cu phases). For the high Mg version of 319 alloy, a single-stage treatment consisting of solutionizing at 510°C for 12–24 h may be recommended. This process should be followed by artificial ageing for 2–5 h at 158°C. Overageing does not bring about much change in the tensile properties.Keywords
This publication has 9 references indexed in Scilit:
- Microstructural aspects of the dissolution and melting of Al2Cu phase in Al-Si alloys during solution heat treatmentMetallurgical and Materials Transactions A, 1996
- Porosity formation in AI-9 Wt Pct Si-3 Wt Pct Cu alloy systems: Metallographic observationsMetallurgical and Materials Transactions A, 1996
- Effect of melt treatment, solidification conditions and porosity level on the tensile properties of 319.2 endchill aluminium castingsJournal of Materials Science, 1995
- A metallographic study of porosity and fracture behavior in relation to the tensile properties in 319.2 end chill castingsMetallurgical and Materials Transactions A, 1995
- The removal of copper-phase segregation and the subsequent improvement in mechanical properties of cast 319 aluminium alloys by a two-stage solution heat treatmentJournal of Materials Processing Technology, 1995
- Heat treatment of 319.2 aluminium automotive alloy Part 2, Ageing behaviourCast Metals, 1995
- Heat treatment of 319.2 aluminium automotive alloy Part 1, Solution heat treatmentCast Metals, 1995
- Effect of magnesium content on the ageing behaviour of water-chilled Al-Si-Cu-Mg-Fe-Mn (380) alloy castingsJournal of Materials Science, 1995
- Effect of alloying elements on the solidification characteristics and microstructure of Al- Si- Cu- Mg- Fe 380 alloyMetallurgical and Materials Transactions A, 1994