Corrosivity of KCl(g) at Temperatures above Its Dew Point - Initial Stages of the High Temperature Corrosion of Alloy Sanicro 28 at 600°C
Authors:
- 15 August 2006
- journal article
- Published by Trans Tech Publications, Ltd. in Materials Science Forum
- Vol. 522-523, 539-546
Abstract
The influence of gaseous KCl on the high temperature oxidation of alloy Sanicro 28 (27Cr31Ni) at 600°C in 5% O2 (N2 in balance) is reported. The samples were exposed isothermally in flowing gas, the dew point of KCl being 590°C corresponding to a partial pressure of KCl of about 2·10-6 atm. The exposure time was 24, 72 and 168 hours. The samples were investigated by gravimetry, grazing incidence XRD, SEM/EDX and AES. The results show that the oxidation of Sanicro 28 at 600°C is accelerated by KCl(g) at metal temperatures above the dew point of the salt. KCl(g) reacts with the protective chromium rich oxide ((Fe1-xCrx)2O3) forming K2CrO4. The resulting chromium depletion of the oxide gives an increasing oxidation rate but does not trigger “breakaway” corrosion. The distribution of potassium chromate on the sample surface is strongly flow-dependent, showing that the rate of formation of potassium chromate is limited by the rate of transport of KCl(g) to the surface. No evidence for chlorine was found on the corroded samples by AES profiling or EDX.Keywords
This publication has 10 references indexed in Scilit:
- Chloridation and oxidation of iron, chromium, nickel and their alloys in chloridizing and oxidizing atmospheres at 400–700°CCorrosion Science, 2000
- The implications of chlorine-associated corrosion on the operation of biomass-fired boilersProgress in Energy and Combustion Science, 2000
- In-situ corrosion investigation at Masnedø CHP plant - a straw-fired power plantMaterials and Corrosion, 1999
- Synergistic Effect of NaCl and Water Vapor on the Corrosion of 1Cr-11Ni-2W-2Mo-V Steel at 500-700°COxidation of Metals, 1999
- Chloridation-oxidation of Fe-Cr and Ni-Cr alloys at 800°COxidation of Metals, 1997
- Corrosion of High Alloy Steels and Fe-Cr-Alloys Beneath Deposits from Waste Incinerator PlantsMaterials Science Forum, 1997
- Thermochemical Data of Pure Substances1995
- The effects of chlorides, hydrogen chloride, and sulfur dioxide in the oxidation of steels below depositsCorrosion Science, 1995
- Hochtemperaturkorrosion des 2.25Cr‐1Mo‐Stahls unter simulierten MüllverbrennungsbedingungenMaterials and Corrosion, 1995
- Accelerated oxidation rate of chromium induced by sodium chlorideOxidation of Metals, 1987