Effect of Si on the Yield Strength of Medium-Carbon Steels Consisting of Ferrite and Pearlite
Open Access
- 5 November 2024
- journal article
- research article
- Published by The Korean Institute of Metals and Materials in Korean Journal of Metals and Materials
- Vol. 62 (11) , 897-910
Abstract
To enhance the intrinsic yield strength of the ferrite-pearlite microstructure that inevitably forms in a non-quenched-and-tempered steel for large structural components, this study analyzed the effect of adding Si. The resulting ferrite-pearlite microstructure in medium-carbon steels was examined, and the resulting increase in yield strength was interpreted based on strengthening mechanisms. Hot-rolled sheets of 0.3C-1.5Mn steels were fabricated with Si ranging from 0.22 to 2.21 wt. %. Austenitization was conducted at 880°C followed by slow continuous cooling, and ferrite-pearlite microstructures were formed. With increasing Si, the yield strength increased from 409.1 to 573.6 MPa. Although there was a negligible change in the austenitic grain size, the mean diameter of the ferritic grains decreased from 8.8 to 5.0 μm, while the mean interlamellar spacing of the pearlites decreased from 196.6 to 109.9 nm. Using these quantitative data about microstructural features and considering possible strengthening mechanisms, a model to predict yield strength was derived via a constrained optimization method. The resulting model indicated that the major mechanisms are the refinement of pearlitic interlamellar spacing and the solid solution strengthening of ferrite by Si. Their contribution to the increment in yield strength was over 75 %, while others such as ferritic grain refinement and increased pearlitic volume fraction have limited influence.Keywords
Funding Information
- Ministry of Trade, Industry and Energy (20022417)
- Korea Planning and Evaluation Institute of Industrial Technology
This publication has 18 references indexed in Scilit:
- Microstructural Characteristics and Strengthening Mechanisms of Ferritic–Martensitic Dual-Phase Steels: A ReviewMetals, 2022
- Development of 1.2 GPa Ferrite-based Lightweight Steels via Low-temperature TemperingKorean Journal of Metals and Materials, 2021
- Influence of Si and Al contents and isothermal treatment condition on the microstructure and tensile properties in ultra-high strength Fe-0.2C-2.0Mn martensite-bainite complex phase steelsKorean Journal of Metals and Materials, 2021
- Physics-informed machine learningNature Reviews Physics, 2021
- Development of an Advanced Ultrahigh Strength TRIP Steel and Evaluation of Its Unique Strain Hardening BehaviorMetals and Materials International, 2019
- Effect of MnS Inclusions Distribution on Intragranular Ferrite Formation in Medium Carbon Non-Quenched and Tempered Steel for Large-Sized CrankshaftISIJ International, 2019
- Effect of Prior Austenite Grain Size on Pearlite Transformation in a Hypoeuctectoid Fe-C-Mn SteelMetallurgical and Materials Transactions A, 2013
- Effect of Silicon Content on the Microstructure and Mechanical Properties of Dual-Phase SteelsMetallography, Microstructure, and Analysis, 2012
- Correlation of Yield Strength and Tensile Strength with Hardness for SteelsJournal of Materials Engineering and Performance, 2008
- Hall–Petch relation and boundary strengtheningScripta Materialia, 2004