Abstract
Corrosion of two multi-phase stainless steels, 17%Cr and 22%Cr, in 15% HCl at temperatures of 80°C and 25°C was studied using mass loss and electrochemical methods. The corrosion environment simulated the environment of acidizing treatment in oil and gas wells. The 17%Cr stainless steel (17Cr steel), consisting of martensite, ferrite, and retained austenite phases, exhibited higher corrosion resistance than the 22%Cr duplex stainless steel (22Cr steel), which consisted of ferrite and austenite phases. In the 22Cr steel, selective corrosion of the ferrite phase was observed. The higher corrosion rate of the 22Cr steel is thought to have been caused by the higher corrosion rate of the ferrite phase, which had a smaller overpotential for the hydrogen evolution reaction. Selective corrosion of the ferrite phase in the 22Cr steel caused detachment of the remaining austenite grains, which also contributed to the higher corrosion rate of the 22Cr steel.