Effect of curing time on the bond strength of a bracket-bonding system cured with a light-emitting diode or plasma arc light
Open Access
- 17 June 2010
- journal article
- research article
- Published by Oxford University Press (OUP) in European Journal of Orthodontics
- Vol. 33 (1) , 55-59
Abstract
The purpose of this study was to assess the influence of two light units, a light-emitting diode (LED) and a plasma arc light (PAC), on the shear bond strength (SBS) of brackets bonded to enamel. Ninety bovine teeth were divided into six groups, according to the light-curing unit and exposure times used. In the LED (Ortholux; 3M-Unitek) group, the specimens were light cured for 5, 10, and 15 seconds. In the PAC (Apollo 95E; DenMed Technologies) group, the specimens were light cured for 3, 6, and 9 seconds. The brackets were bonded with Transbond XT (3M-Unitek), stored in distilled water at 37°C for 24 hours and then submitted to SBS testing in a universal testing machine. The adhesive remnant index (ARI) was used to evaluate the amount of adhesive remaining on the teeth. According to analysis of variance and Tukey multiple comparisons test, the highest mean SBS was obtained with the LED at 15 seconds (16.68 MPa), which did not significantly differ from the LED 10 (14.76 MPa) or 5 (13.92 MPa) second groups (P > 0.05). The LED 10 and 5 second groups were not significantly different from the PAC 9 second group (12.66 MPa) or from the PAC 6 second group (9.96 MPa). The lowest mean SBS was obtained with the PAC 3 second group (8.29 MPa), which did not differ significantly from the PAC 6 second group. The method of light curing did not influence the ARI, with score 3 predominant. The LED at 5 seconds and the PAC at 3 seconds provided sufficient mean SBS to resist either orthodontic or masticatory forces.Keywords
This publication has 33 references indexed in Scilit:
- Light curing time reduction: in vitro evaluation of new intensive light-emitting diode curing unitsEuropean Journal of Orthodontics, 2005
- Plasma arc versus halogen light-curing of adhesive-precoated orthodontic brackets: A 12-month clinical study of bond failuresAmerican Journal of Orthodontics and Dentofacial Orthopedics, 2004
- Plasma arc curing lights for orthodontic bondingAmerican Journal of Orthodontics and Dentofacial Orthopedics, 2002
- Polymerization of orthodontic resin cement with light-emitting diode curing unitsAmerican Journal of Orthodontics and Dentofacial Orthopedics, 2002
- The inappropriateness of conventional orthodontic bond strength assessment protocolsEuropean Journal of Orthodontics, 2000
- Depth of cure and compressive strength of dental composites cured with blue light emitting diodes (LEDs)Dental Materials, 2000
- Structural conformation of in vitro and in vivo aged orthodontic elastomeric modulesEuropean Journal of Orthodontics, 1999
- Dental composite depth of cure with halogen and blue light emitting diode technologyBritish Dental Journal, 1999
- Clinical trials with crystal growth conditioning as an alternative to acid-etch enamel pretreatmentAmerican Journal of Orthodontics, 1984
- A Simple Method of Increasing the Adhesion of Acrylic Filling Materials to Enamel SurfacesJournal of Dental Research, 1955