Early bond strength of two resin cements to Y-TZP ceramic using MPS or MPS/4-META silanes
- 27 January 2011
- journal article
- research article
- Published by Springer Nature in Odontology
- Vol. 99 (1) , 62-67
Abstract
For cementation of yttrium-stabilized tetragonal zirconium polycrystal (Y-TZP) ceramic frameworks, protocols of surface-conditioning methods and available cements vary, resulting in confusion among clinicians regarding selection and effects of different conditioning methods on cement adhesion. This study evaluated the effect of two silanes (3-trimethoxysilylpropylmethacrylate (MPS) and 3-trimethoxysilylpropylmethacrylate/4-methacryloyloxyethyl trimellitate anhydride methyl methacrylate (MPS/4-META) on the adhesion of two resin-based cements (SuperBond and Panavia F 2.0) to Y-TZP ceramic and compared several protocols with those indicated by the manufacturer of each of these cements. Disks of Y-TZP ceramic (LAVA, 3M ESPE) (n = 60) were divided into six experimental groups (n = 10 per group) and treated as follows: (1) silica coating (SC) + MPS silane + SuperBond; (2) SC + MPS/4-META + silane + SuperBond); (3) SC + MPS silane + Panavia F 2.0); (4) SC + MPS/4-META silane + Panavia F 2.0); (5) no conditioning + MPS/4-META silane + Super-Bond (SuperBond instructions); and (6) 50-μm Al2O3 conditioning + Panavia F 2.0 (Panavia F 2.0 instructions). The specimens were subjected to shear-bond testing after water storage at 37°C for 3 months in the dark. Data were analyzed by analysis of variance and Tukey’s HSD (α = 0.05). After silica coating, the mean bond strength of SuperBond cement was not significantly different between MPS and MPS/4-META silanes (20.2 ± 3.7 and 20.9 ± 1.6 MPa, respectively), but the mean bond strength of Panavia F 2.0 was significantly higher with MPS silane (24.4 ± 5.3 MPa) than with MPS/4-META (12.3 ± 1.4 MPa) (P < 0.001). The SuperBond manufacturer’s instructions alone resulted in significantly higher bond strength (9.7 ± 3.1 MPa) than the Panavia F 2.0 manufacturer’s instruction (0 MPa) (P < 0.001). When silica coating and silanization were used, both SuperBond and Panavia F 2.0 cements demonstrated higher bond strengths they did when the manufacturers’ instructions were followed. With SuperBond, use of MPS or MPS/4-META silane resulted in no significant difference when the ceramic surface was silica coated, but with Panavia F 2.0, use of MPS silane resulted in a significantly higher bond strength than use of MPS/4-META. Use of chairside silica coating and silanization to condition the zirconia surface improved adhesion compared with the manufacturers’ cementation protocols for SuperBond and Panavia F 2.0 resin cements.Keywords
This publication has 24 references indexed in Scilit:
- To what extent does the longevity of fixed dental prostheses depend on the function of the cement? Working Group 4 materials: cementationClinical Oral Implants Research, 2007
- The efficacy of posterior three-unit zirconium-oxide–based ceramic fixed partial dental prostheses: A prospective clinical pilot studyThe Journal of Prosthetic Dentistry, 2006
- Microtensile bond strength of a resin cement to glass infiltrated zirconia-reinforced ceramic: The effect of surface conditioningDental Materials, 2006
- Bonding of dual‐cured resin cement to zirconia ceramic using phosphate acid ester monomer and zirconate couplerJournal of Biomedical Materials Research Part B: Applied Biomaterials, 2005
- Fatigue and damage tolerance of Y‐TZP ceramics in layered biomechanical systemsJournal of Biomedical Materials Research Part B: Applied Biomaterials, 2004
- Strength, fracture toughness and microstructure of a selection of all-ceramic materials. Part II. Zirconia-based dental ceramicsDental Materials, 2004
- Resin-ceramic bonding: A review of the literatureThe Journal of Prosthetic Dentistry, 2003
- Hydrolytic stability of silanated zirconia‐silica‐urethane dimethacrylate compositesJournal of Oral Rehabilitation, 1995
- Studies of the simulation of silane coupling agent structures on particulate fillers; the pH effectPolymer Composites, 1984
- Adhesion Through Silane Coupling AgentsThe Journal of Adhesion, 1970