Abstract
The pursuit of sustainable thermoelectric materials requires the development of cost-effective and efficient compounds derived from earth-abundant elements. Here, we investigate the effects of samarium (Sm) substitution on the thermoelectric performance of SrSi₂ with compositions Sr1-xSmxSi2 (x = 0, 0.05, 0.1, 0.15, and 0.2). Substituting Sm for Sr in SrSi₂ enhances the power factor at low substitution levels, while further substitution leads to a decrease, due to increased carrier scattering and reduced Seebeck coefficient. Introducing Sm substitution enhances phonon scattering through point defects, reducing lattice thermal conductivity. A peak figure of merit (ZT) of ~0.23 at room temperature is achieved for Sr₀.₉₅Sm₀.₀₅Si₂, demonstrating a 35% improvement over undoped SrSi₂. The weighted mobility of ~285 cm2/V·s and the tailored thermal transport emphasize the role of Sm substitution in modulating both electronic and thermal properties. These findings establish Sr1-xSmxSi2 as a promising candidate for next-generation thermoelectric devices.
Funding Information
  • JST-Mirai Program (JPMJMI19A1)
  • Japan Society for the Promotion of Science (24K21692)
  • Japan Society for the Promotion of Science (24K00590)

This publication has 65 references indexed in Scilit: