Adhesive bond strength of monolithic zirconia ceramic finished with various surface treatments
Authors:
Open Access
- 13 November 2023
- journal article
- research article
- Published by Springer Nature in BMC Oral Health
- Vol. 23 (1) , 1-10
Abstract
Background: This study aimed to investigate different surface treatments thought to increase the bond strength between zirconia ceramic and adhesive resin cement. Methods: The samples were prepared in 15 × 10 × 2 mm dimensions by cutting off monolithic zirconia ceramic blocks (Incoris TZI; Sirona, Germany). Surface roughness measurements were made with a profilometer, the average surface roughness (Ra1) was recorded, and five different surface treatments were applied. Group 1: Control group. No surface treatment was applied. Group 2: Sandblasted with Al2O3 under pressure of 50 μm. Group 3: Sandblasted with 30 μm Al2O3 - SiOx under pressure, then tribochemical silica coating, silane bonding agent, and ceramic primer were applied. Group 4: Samples were etched in a hot acid solution containing methanol, HCl, and chloride at 100 °C. Group 5: Samples were coated in a solution containing Grade C Aluminum Nitrite at 75 °C for 15 Sects. 12,000 thermal aging was carried out to all samples. Then, samples were bonded to a composite surface (Filtek Z250) with two different types of adhesive cement (Panavia F 2.0, Rely X U200) (n = 10). A load was applied to the samples attached to the Universal Test Device for the SBS, and the SBS was recorded. The surface roughness measurements of all samples were made again, and the average surface roughness Ra2 was recorded. The data was analyzed with a two-way ANOVA test. Bonferroni correction was used for multiple comparisons of the groups. p = 0.005 was accepted as the statistically significant value. Results: There was no statistically significant difference between the groups in the Ra1 measurements (p = 0.031). There was a statistically significant difference between the Ra2 values of Groups 4 and 5 and the Ra2 values of Groups 1,2 and 3 in the Ra2 measurements (p < 0.001). There was no statistically significant difference between the SBS values of the groups (p > 0.005). Also, there was no statistically significant difference in the SBS values of all groups for the two different cements tested (p > 0.005). Conclusions: None of the surface treatments applied to monolithic zirconia ceramic samples increased the SBS between ceramic and adhesive resin cement.Keywords
This publication has 37 references indexed in Scilit:
- Thermocycling effect on microshear bond strength to zirconia ceramic using Er:YAG and tribochemical silica coating as surface conditioningLasers in Medical Science, 2013
- Shear Bond Strength of Resin Cement to Zirconia Ceramic After Aluminum Oxide Sandblasting and Various Laser TreatmentsPhotomedicine and Laser Surgery, 2011
- Cements and Adhesives for All-Ceramic RestorationsDental Clinics of North America, 2011
- Adhesion/cementation to zirconia and other non-silicate ceramics: Where are we now?Dental Materials, 2011
- The Effect of Laser Treatment on Bonding Between Zirconia Ceramic Surface and Resin CementActa Odontologica Scandinavica, 2010
- Innovations in bonding to zirconia based ceramics: Part III. Phosphate monomer resin cementsDental Materials, 2010
- Morphological analysis of three zirconium oxide ceramics: Effect of surface treatmentsDental Materials, 2010
- Surface modification for enhanced silanation of zirconia ceramicsDental Materials, 2009
- Comparison of resin cement adhesion to Y-TZP ceramic following manufacturers’ instructions of the cements onlyClinical Oral Investigations, 2007
- Microtensile bond strength of a resin cement to glass infiltrated zirconia-reinforced ceramic: The effect of surface conditioningDental Materials, 2006