A Proposal for the Application of Failure Assessment Diagrams to Subcritical Hydrogen Induced Cracking Propagation Processes
Authors:
- Borja Arroyo MartínezBMBorja Arroyo Martínez
- José Alberto Álvarez LasoJLJosé Alberto Álvarez Laso
- Federico Gutiérrez-SolanaFGFederico Gutiérrez-Solana
- Alberto Cayón MartínezAMAlberto Cayón Martínez
- Yahoska Julieth Jirón MartínezYMYahoska Julieth Jirón Martínez
- Ana Ruht Seco AparicioAAAna Ruht Seco Aparicio
Open Access
Abstract
In this work, an optimization proposal for a model based on the definition of regions for crack propagation by means of the micromechanical comparison by SEM images and its application to failure assessment diagrams (FADs) is presented. It consists in three approaches. (1) The definition of the crack propagation initiation in the elastic-plastic range. (2) A slight modification of the zones in which the FAD is divided for hydrogen induced cracking (HIC) conditions. (3) The introduction of a simple correction for the definition of the Kr coordinate of the FAD to take into account the fracture toughness reduction caused by an aggressive environment, instead of using a fracture parameter obtained from a test in air. For the experimental work, four medium and high strength steels exposed to a cathodic charge and cathodic protection environments were employed, studying two different loading rates in each case, and testing C(T) samples under slow rates in the environment. The study was completed with a subsequent fractographic analysis by SEM. A good degree of fulfilment was appreciated in both materials and environmental conditions, showing the validity of the predictions supplied by the FAD optimization model proposal, which constitutes an advance in the accuracy of the FAD predictive model.Keywords
Funding Information
- Ministerio de Asuntos Económicos y Transformación Digital, Gobierno de España (MAT2014-58738-C3-3-R)
- CECA (7210-PE/110)
- Universidad de Cantabria (62.0000.64251)
This publication has 11 references indexed in Scilit:
- A Theory of Critical Distances based methodology for the analysis of environmentally assisted cracking in steelsEngineering Fracture Mechanics, 2019
- Analysis of key factors of hydrogen environmental assisted cracking evaluation by small punch test on medium and high strength steelsMaterials Science and Engineering: A, 2017
- Study of the energy for embrittlement damage initiation by SPT means. Estimation of KEAC in aggressive environments and rate considerationsTheoretical and Applied Fracture Mechanics, 2016
- Hydrogen in Metals2014
- Probabilistic Transgranular Stress Corrosion Cracking Analysis for Oil and Gas PipelinesJournal of Pressure Vessel Technology, 2012
- The Metal-Hydrogen System2005
- An elastic–plastic fracture mechanics based methodology to characterize cracking behavior and its application to environmental assisted processesNuclear Engineering and Design, 1999
- A strain-based fracture model for stress corrosion cracking of low-alloy steelsMetallurgical and Materials Transactions A, 1996
- A SUMMARY REPORT OF AN ESIS WORKING PARTY ON FRACTURE CONTROL GUIDELINES FOR ENVIRONMENTALLY ASSISTED CRACKING OF LOW ALLOY STEELSFatigue & Fracture of Engineering Materials & Structures, 1993
- Advances in Corrosion Science and Technology1980