Influence of solutioning and ageing heat treatments on microstructure, mechanical properties, and tribological behavior of Ti-6Al-5Zr-0.5Mo-0.2Si alloy
Open Access
- 1 January 2025
- journal article
- Published by FapUNIFESP (SciELO) in Matéria (Rio de Janeiro)
- Vol. 30
Abstract
The present study investigates the effect of heat treatment on the microstructure, mechanical, and wear characteristics of the Ti-6Al-5Zr-0.5Mo-0.2Si alloy. Solution heat treatment combined with aging near the β-transus temperature substantially modified the microstructure, resulting in notable enhancements in the mechanical properties. Solution annealing followed by ageing at 1050°C was highly effective, as it formed secondary α phases near the retained β phase. This refined microstructure contributed to a notable increase in tensile strength, achieving a higher strength of 1270 ± 10 MPa (29% more) and a microhardness of 360 ± 5 HV (14% more) than the as-received base material through transformation strengthening mechanisms. Additionally, the heat-treated alloys demonstrated superior wear resistance compared to their as-received condition. High-temperature wear testing at 200 °C showed the formation of a stable tribo-oxide layer on the alloy surface, which acted as a protective barrier against direct metal-to-metal contact. This layer significantly enhanced wear resistance, reaching 4.39 × 10−3 mm3/Nm, an improvement of 33% over the as-received base metal.Keywords
This publication has 36 references indexed in Scilit:
- RETRACTED ARTICLE: Comparative analysis of solution treatment with short and long-term aging on mechanical, tribological, and corrosion potential of Ti-6Al-4V alloyMultiscale and Multidisciplinary Modeling, Experiments and Design, 2025
- Effect of Solution Treatment and Aging Temperature on α′ and Ti3Al(α2) Phase Formation and Mechanical Properties of Water-Quenched Ti–6Al–4VMetallography, Microstructure, and Analysis, 2022
- Correction to: Effect of Strain Hardening and Aging Processes on Microstructure Evolution, Tensile and Fatigue Properties of Cast Ti-6Al-2Sn-2Zr–2Mo-1.5Cr-2Nb-0.1Si AlloyInternational Journal of Metalcasting, 2021
- Microstructural evolution and mechanical properties of selective laser melted Ti-6Al-4V induced by annealing treatmentJournal of Central South University, 2021
- Phase transformation and its effect on mechanical characteristics in warm-deformed Ti-29Nb-13Ta-4.6Zr alloyMetals and Materials International, 2015
- Analysis for Wear Behaviors of Oxidative WearTribology Letters, 2011
- On the occurrence of dynamic strain aging in near-alpha alloy Ti-5.8Al-4Sn-3.5Zr-0.7Nb-0.5Mo-0.35SiMetallurgical and Materials Transactions A, 1999
- Microstructure, tensile deformation, and fracture in aged ti 10V-2Fe-3AlMetallurgical Transactions A, 1983
- Material transport phenomena in the impact wear of titanium alloysWear, 1980
- Silicide precipitation in the Ti−Zr−Al−Si systemMetallurgical Transactions, 1971