Influence of Cryogenic Treatment on the Tribological Properties of High-Chromium White Cast Iron

Authors:

Abstract
This study examines the impact of cryogenic treatment on the tribological properties of High-Chromium White Cast Iron (HCWCI), a material widely used in mining and shot blasting equipment due to its excellent abrasive wear resistance. The main challenge with this material is the as-cast microstructure, which contains a high-volume fraction (~55.6%) of retained austenite, a soft phase (374 HV0.05) that reduces wear resistance. The research applied sequential heat treatments: quenching, deep cryogenic treatment (4 hours in liquid nitrogen), and tempering. Wear resistance was evaluated using a rubber-wheel abrasive tribometer (ASTM G65) and field testing in blast turbine operations (900 hours). Results confirmed that cryogenic treatment effectively transformed retained austenite into martensite and promoted fine secondary carbide precipitation. Results confirmed carbide precipitation, supporting the treatment’s role in enhancing wear resistance. Optical and scanning electron microscopy, and retained austenite were quantified by X-ray diffraction. Microstructural analysis confirmed carbide precipitation, supporting the treatment's role in enhancing wear resistance. Cryogenic treatment effectively transformed retained austenite into martensite and promoted fine secondary carbide precipitation. This microstructural evolution led to a dramatic increase in hardness: overall hardness rose from 50 HRC (as-cast) to 66 HRC after treatment, with matrix microhardness reaching 914 HV(0.05). Consequently, performance tests showed a 46% improvement in wear resistance for cryogenically treated and tempered samples.