Abstract
Single-phase of CaLn1−xAl3O7:xTb3+(Ln=La,Gd,0≤x≤1)CaLn1−xAl3O7:xTb3+(Ln=La,Gd,0≤x≤1) was synthesized by citric-gel processing and photoluminescence (PL) properties in the range of 125–300nm125–300nm were investigated. The bands below 200nm200nm with maxima at approximately 180nm180nm in excitation spectra were assigned to the host lattice absorption, the bands above 200nm200nm with a maximum at about 235 and 237nm237nm in CaLa1−xAl3O7:xTb3+CaLa1−xAl3O7:xTb3+ and CaGd1−xAl3O7:xTb3+CaGd1−xAl3O7:xTb3+ , respectively, corresponding to 4f8→4f75d14f8→4f75d1 transition of Tb3+Tb3+ . The phosphors exhibited a strong emission at around 543nm543nm under 147147 and 254nm254nm excitation corresponding to the D45→F57D45→F57 transition of Tb3+Tb3+ . Optimal emission intensity was obtained at x=0.8x=0.8 under 254nm254nm excitation and at x=0.2x=0.2 under 147nm147nm excitation in CaLn1−xAl3O7:xTb3+(Ln=La,Gd)CaLn1−xAl3O7:xTb3+(Ln=La,Gd) . The calculated luminescent chromaticity coordinates were (0.340, 0.559) and (0.337, 0.523) in Ca(Tb0.2La0.8)Al3O7Ca(Tb0.2La0.8)Al3O7 and Ca(Tb0.2Gd0.8)Al3O7Ca(Tb0.2Gd0.8)Al3O7 under 147nm147nm excitation.

This publication has 14 references indexed in Scilit: